did anybody ever see any defects like this on the resist surface
after resist spinning. The diameter varies from about 20um to over
150um.<br>
<br>
<img src="cid:part1.51001AC2.15A95466@gno.de" alt=""><br>
<br>
<img src="cid:part2.4437EB4D.6D9807A5@gno.de" alt=""><br>
<br>
<br>
Any idea what the reason could be?<br>