<div dir="ltr"><div>The same situation there. We were asked for Ir sputtering last month. The cost of a 3 inch target is more than $100,000 from the quote that we got from a supplier. That stops us from proceeding with the project. <br></div><div dir="ltr"><br></div><div>Best,</div><div>Chao</div><div dir="ltr"><br></div><div dir="ltr">--</div><div dir="ltr"><br><div dir="ltr" class="gmail_signature"><div dir="ltr"><div dir="ltr"><div dir="ltr"><div dir="ltr"><font color="#0b5394"><img src="https://drive.google.com/uc?id=1VsUYvli9WeVR0tCaW1bQEncBtx6nEOsd&export=download" width="96" height="95"><br></font></div><div dir="ltr"><font face="monospace" color="#0b5394" size="4"><b>Zhichao (Chao) Wang, Ph.D.</b></font></div><div dir="ltr"><i><font color="#0b5394" face="trebuchet ms, sans-serif">Nano Process Specialist</font></i></div><div dir="ltr"><font color="#0b5394" face="trebuchet ms, sans-serif"><i>UDNF</i></font></div><div><font color="#0b5394" face="trebuchet ms, sans-serif"><i>University of Delaware</i></font></div><div><font face="trebuchet ms, sans-serif"><i><font color="#0b5394">Pronouns: He/Him/His</font></i><font color="#0b5394"><i><br></i></font></font></div><div><i><font color="#0b5394" face="trebuchet ms, sans-serif"><span style="font-size:12px">------------------------</span></font></i></div><div dir="ltr"><i><font color="#0b5394" face="trebuchet ms, sans-serif">Office Number:(302) 831-4839</font></i></div><div dir="ltr"><font color="#0b5394" face="trebuchet ms, sans-serif"><i>221 Academy St.,RM170</i></font></div><div dir="ltr"><font color="#0b5394" face="trebuchet ms, sans-serif"><i>Newark, DE 19711</i></font></div></div></div></div></div></div><div dir="ltr"><div dir="ltr"><br></div><br><div class="gmail_quote"><div dir="ltr" class="gmail_attr">On Wed, Apr 20, 2022 at 1:11 PM Aebersold,Julia W. <<a href="mailto:julia.aebersold@louisville.edu" target="_blank">julia.aebersold@louisville.edu</a>> wrote:<br></div><blockquote class="gmail_quote" style="margin:0px 0px 0px 0.8ex;border-left:1px solid rgb(204,204,204);padding-left:1ex">
<div lang="EN-US">
<div>
<p class="MsoNormal">We were also asked to deposit iridium last year and the cost of the 3” target immediately stopped the project.
<u></u><u></u></p>
<p class="MsoNormal"><u></u> <u></u></p>
<div>
<p class="MsoNormal"><span style="color:black">Cheers!<u></u><u></u></span></p>
<p class="MsoNormal"><span style="color:black"><u></u> <u></u></span></p>
<p class="MsoNormal"><span style="color:black">Julia Aebersold, Ph.D.</span><span style="font-size:12pt;font-family:"Times New Roman",serif;color:black"><u></u><u></u></span></p>
<p class="MsoNormal"><span style="color:black">Manager, Micro/Nano Technology Center</span><span style="font-size:12pt;font-family:"Times New Roman",serif;color:black"><u></u><u></u></span></p>
<p class="MsoNormal"><span style="color:black">University of Louisville</span><span style="font-size:12pt;font-family:"Times New Roman",serif;color:black"><u></u><u></u></span></p>
<p class="MsoNormal"><span style="color:black">Shumaker Research Building, Room 233</span><span style="font-size:12pt;font-family:"Times New Roman",serif;color:black"><u></u><u></u></span></p>
<p class="MsoNormal"><span style="color:black">2210 South Brook Street</span><span style="font-size:12pt;font-family:"Times New Roman",serif;color:black"><u></u><u></u></span></p>
<p class="MsoNormal"><span style="color:black">Louisville, KY 40292</span><span style="font-size:12pt;font-family:"Times New Roman",serif;color:black"><u></u><u></u></span></p>
<p class="MsoNormal"><span style="color:black">(502) 852-1572</span><span style="font-size:12pt;font-family:"Times New Roman",serif;color:black"><u></u><u></u></span></p>
<p class="MsoNormal"><span style="color:black"> </span><span style="font-size:12pt;font-family:"Times New Roman",serif;color:black"><u></u><u></u></span></p>
<p class="MsoNormal"><span style="color:black"><a href="http://louisville.edu/micronano/" target="_blank"><span style="color:black">http://louisville.edu/micronano/</span></a></span><span style="color:black"><u></u><u></u></span></p>
</div>
<p class="MsoNormal"><u></u> <u></u></p>
<div>
<div style="border-right:none;border-bottom:none;border-left:none;border-top:1pt solid rgb(225,225,225);padding:3pt 0in 0in">
<p class="MsoNormal"><b>From:</b> labnetwork <<a href="mailto:labnetwork-bounces@mtl.mit.edu" target="_blank">labnetwork-bounces@mtl.mit.edu</a>> <b>
On Behalf Of </b>Brian K. Olmsted<br>
<b>Sent:</b> Tuesday, April 19, 2022 1:03 PM<br>
<b>To:</b> <a href="mailto:labnetwork@mtl.mit.edu" target="_blank">labnetwork@mtl.mit.edu</a><br>
<b>Subject:</b> [labnetwork] Iridium sputter target?<u></u><u></u></p>
</div>
</div>
<p class="MsoNormal"><u></u> <u></u></p>
<p class="MsoNormal" style="line-height:12pt;background:rgb(255,77,77)">
<b><span style="font-size:10pt;color:black">CAUTION:</span></b><span style="font-size:10pt;color:black"> This email originated from outside of our organization. Do not click links, open attachments, or respond unless you recognize the sender's email address
and know the contents are safe.</span><u></u><u></u></p>
<div>
<div>
<p class="MsoNormal">Hi, <u></u><u></u></p>
<div>
<p class="MsoNormal"><u></u> <u></u></p>
</div>
<div>
<p class="MsoNormal">I've got a prospective customer interested in sputtering iridium. We don't have an iridium target and it probably doesn't make a lot of sense for us to purchase one for extremely limited interest/use. However, if there is another lab that
has this capability I would be happy to steer them to you for at least this step in their process.<u></u><u></u></p>
</div>
<div>
<p class="MsoNormal"><u></u> <u></u></p>
</div>
<div>
<p class="MsoNormal">Any information or help is appreciated.<u></u><u></u></p>
</div>
<div>
<p class="MsoNormal"><u></u> <u></u></p>
</div>
<div>
<p class="MsoNormal">Thanks,<u></u><u></u></p>
</div>
<div>
<p class="MsoNormal"><br clear="all">
<u></u><u></u></p>
<div>
<div>
<div>
<div>
<p class="MsoNormal">Brian K. Olmsted<u></u><u></u></p>
</div>
<div>
<p class="MsoNormal">Associate Director of Laboratory Operations<u></u><u></u></p>
<div>
<p class="MsoNormal">University of Minnesota | MNC<u></u><u></u></p>
<div>
<p class="MsoNormal"><a href="https://nam11.safelinks.protection.outlook.com/?url=http%3A%2F%2Fwww.mnc.umn.edu%2F&data=05%7C01%7Cjulia.aebersold%40louisville.EDU%7C4f913867e16e4490ad5208da2255449c%7Cdd246e4a54344e158ae391ad9797b209%7C0%7C0%7C637860046892720519%7CUnknown%7CTWFpbGZsb3d8eyJWIjoiMC4wLjAwMDAiLCJQIjoiV2luMzIiLCJBTiI6Ik1haWwiLCJXVCI6Mn0%3D%7C1000%7C%7C%7C&sdata=ICuT4PHPzPsTsBRbIAegatGo%2FFAg%2F0EKhkc5Vt0Uisk%3D&reserved=0" target="_blank">www.mnc.umn.edu</a><u></u><u></u></p>
</div>
</div>
<div>
<p class="MsoNormal">612.626.3287<u></u><u></u></p>
</div>
<div>
<p class="MsoNormal"><a href="mailto:olms0025@umn.edu" target="_blank">olms0025@umn.edu</a><u></u><u></u></p>
</div>
<div>
<p class="MsoNormal"><u></u> <u></u></p>
</div>
</div>
</div>
</div>
</div>
</div>
</div>
</div>
</div>
</div>
_______________________________________________<br>
labnetwork mailing list<br>
<a href="mailto:labnetwork@mtl.mit.edu" target="_blank">labnetwork@mtl.mit.edu</a><br>
<a href="https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork" rel="noreferrer" target="_blank">https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork</a><br>
</blockquote></div></div>
</div>