    What we do at CNS is to run a sub-atmospheric regulator on BCl3, so
    that we don't have to run any heating tape on the lines.  As long as
    the supply lines are not so long that elevated pressure is needed to
    generate the needed flow rate, running the regulator below
    atmospheric pressure avoids condensation, without the need for
    supplemental heat.<br>
    <br>
    <br>
    Mac<br>
    <br>
    <br>
    <div class="moz-signature">
      
      <meta name="ProgId" content="Word.Document">
      <meta name="Generator" content="Microsoft Word 14">
      <meta name="Originator" content="Microsoft Word 14">
      <link rel="File-List" href="Mac%20Hathaway%20Email%20Signature%20File_files/filelist.xml">
      <!--[if gte mso 9]><xml>
 <o:DocumentProperties>
  <o:Author>Mac</o:Author>
  <o:LastAuthor>Mac</o:LastAuthor>
  <o:Revision>2</o:Revision>
  <o:TotalTime>1</o:TotalTime>
  <o:Created>2014-07-10T20:07:00Z</o:Created>
  <o:LastSaved>2014-07-10T20:07:00Z</o:LastSaved>
  <o:Pages>1</o:Pages>
  <o:Words>20</o:Words>
  <o:Characters>115</o:Characters>
  <o:Company>Harvard University</o:Company>
  <o:Lines>1</o:Lines>
  <o:Paragraphs>1</o:Paragraphs>
  <o:CharactersWithSpaces>134</o:CharactersWithSpaces>
  <o:Version>14.00</o:Version>
 </o:DocumentProperties>
 <o:OfficeDocumentSettings>
  <o:AllowPNG/>
 </o:OfficeDocumentSettings>
</xml><![endif]-->
      <link rel="themeData" href="Mac%20Hathaway%20Email%20Signature%20File_files/themedata.thmx">
      <link rel="colorSchemeMapping" href="Mac%20Hathaway%20Email%20Signature%20File_files/colorschememapping.xml">
      <!--[if gte mso 9]><xml>
 <w:WordDocument>
  <w:SpellingState>Clean</w:SpellingState>
  <w:GrammarState>Clean</w:GrammarState>
  <w:TrackMoves>false</w:TrackMoves>
  <w:TrackFormatting/>
  <w:PunctuationKerning/>
  <w:ValidateAgainstSchemas/>
  <w:SaveIfXMLInvalid>false</w:SaveIfXMLInvalid>
  <w:IgnoreMixedContent>false</w:IgnoreMixedContent>
  <w:AlwaysShowPlaceholderText>false</w:AlwaysShowPlaceholderText>
  <w:DoNotPromoteQF/>
  <w:LidThemeOther>EN-US</w:LidThemeOther>
  <w:LidThemeAsian>X-NONE</w:LidThemeAsian>
  <w:LidThemeComplexScript>X-NONE</w:LidThemeComplexScript>
  <w:Compatibility>
   <w:BreakWrappedTables/>
   <w:SnapToGridInCell/>
   <w:WrapTextWithPunct/>
   <w:UseAsianBreakRules/>
   <w:DontGrowAutofit/>
   <w:DontUseIndentAsNumberingTabStop/>
   <w:FELineBreak11/>
   <w:WW11IndentRules/>
   <w:DontAutofitConstrainedTables/>
   <w:AutofitLikeWW11/>
   <w:HangulWidthLikeWW11/>
   <w:UseNormalStyleForList/>
   <w:DontVertAlignCellWithSp/>
   <w:DontBreakConstrainedForcedTables/>
   <w:DontVertAlignInTxbx/>
   <w:Word11KerningPairs/>
   <w:CachedColBalance/>
  </w:Compatibility>
  <m:mathPr>
   <m:mathFont m:val="Cambria Math"/>
   <m:brkBin m:val="before"/>
   <m:brkBinSub m:val="--"/>
   <m:smallFrac m:val="off"/>
   <m:dispDef/>
   <m:lMargin m:val="0"/>
   <m:rMargin m:val="0"/>
   <m:defJc m:val="centerGroup"/>
   <m:wrapIndent m:val="1440"/>
   <m:intLim m:val="subSup"/>
   <m:naryLim m:val="undOvr"/>
  </m:mathPr></w:WordDocument>
</xml><![endif]--><!--[if gte mso 9]><xml>
 <w:LatentStyles DefLockedState="false" DefUnhideWhenUsed="true"
  DefSemiHidden="true" DefQFormat="false" DefPriority="99"
  LatentStyleCount="267">
  <w:LsdException Locked="false" Priority="0" SemiHidden="false"
   UnhideWhenUsed="false" QFormat="true" Name="Normal"/>
  <w:LsdException Locked="false" Priority="9" SemiHidden="false"
   UnhideWhenUsed="false" QFormat="true" Name="heading 1"/>
  <w:LsdException Locked="false" Priority="9" QFormat="true" Name="heading 2"/>
  <w:LsdException Locked="false" Priority="9" QFormat="true" Name="heading 3"/>
  <w:LsdException Locked="false" Priority="9" QFormat="true" Name="heading 4"/>
  <w:LsdException Locked="false" Priority="9" QFormat="true" Name="heading 5"/>
  <w:LsdException Locked="false" Priority="9" QFormat="true" Name="heading 6"/>
  <w:LsdException Locked="false" Priority="9" QFormat="true" Name="heading 7"/>
  <w:LsdException Locked="false" Priority="9" QFormat="true" Name="heading 8"/>
  <w:LsdException Locked="false" Priority="9" QFormat="true" Name="heading 9"/>
  <w:LsdException Locked="false" Priority="39" Name="toc 1"/>
  <w:LsdException Locked="false" Priority="39" Name="toc 2"/>
  <w:LsdException Locked="false" Priority="39" Name="toc 3"/>
  <w:LsdException Locked="false" Priority="39" Name="toc 4"/>
  <w:LsdException Locked="false" Priority="39" Name="toc 5"/>
  <w:LsdException Locked="false" Priority="39" Name="toc 6"/>
  <w:LsdException Locked="false" Priority="39" Name="toc 7"/>
  <w:LsdException Locked="false" Priority="39" Name="toc 8"/>
  <w:LsdException Locked="false" Priority="39" Name="toc 9"/>
  <w:LsdException Locked="false" Priority="35" QFormat="true" Name="caption"/>
  <w:LsdException Locked="false" Priority="10" SemiHidden="false"
   UnhideWhenUsed="false" QFormat="true" Name="Title"/>
  <w:LsdException Locked="false" Priority="1" Name="Default Paragraph Font"/>
  <w:LsdException Locked="false" Priority="11" SemiHidden="false"
   UnhideWhenUsed="false" QFormat="true" Name="Subtitle"/>
  <w:LsdException Locked="false" Priority="22" SemiHidden="false"
   UnhideWhenUsed="false" QFormat="true" Name="Strong"/>
  <w:LsdException Locked="false" Priority="20" SemiHidden="false"
   UnhideWhenUsed="false" QFormat="true" Name="Emphasis"/>
  <w:LsdException Locked="false" Priority="59" SemiHidden="false"
   UnhideWhenUsed="false" Name="Table Grid"/>
  <w:LsdException Locked="false" UnhideWhenUsed="false" Name="Placeholder Text"/>
  <w:LsdException Locked="false" Priority="1" SemiHidden="false"
   UnhideWhenUsed="false" QFormat="true" Name="No Spacing"/>
  <w:LsdException Locked="false" Priority="60" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light Shading"/>
  <w:LsdException Locked="false" Priority="61" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light List"/>
  <w:LsdException Locked="false" Priority="62" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light Grid"/>
  <w:LsdException Locked="false" Priority="63" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Shading 1"/>
  <w:LsdException Locked="false" Priority="64" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Shading 2"/>
  <w:LsdException Locked="false" Priority="65" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium List 1"/>
  <w:LsdException Locked="false" Priority="66" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium List 2"/>
  <w:LsdException Locked="false" Priority="67" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 1"/>
  <w:LsdException Locked="false" Priority="68" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 2"/>
  <w:LsdException Locked="false" Priority="69" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 3"/>
  <w:LsdException Locked="false" Priority="70" SemiHidden="false"
   UnhideWhenUsed="false" Name="Dark List"/>
  <w:LsdException Locked="false" Priority="71" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful Shading"/>
  <w:LsdException Locked="false" Priority="72" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful List"/>
  <w:LsdException Locked="false" Priority="73" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful Grid"/>
  <w:LsdException Locked="false" Priority="60" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light Shading Accent 1"/>
  <w:LsdException Locked="false" Priority="61" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light List Accent 1"/>
  <w:LsdException Locked="false" Priority="62" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light Grid Accent 1"/>
  <w:LsdException Locked="false" Priority="63" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Shading 1 Accent 1"/>
  <w:LsdException Locked="false" Priority="64" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Shading 2 Accent 1"/>
  <w:LsdException Locked="false" Priority="65" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium List 1 Accent 1"/>
  <w:LsdException Locked="false" UnhideWhenUsed="false" Name="Revision"/>
  <w:LsdException Locked="false" Priority="34" SemiHidden="false"
   UnhideWhenUsed="false" QFormat="true" Name="List Paragraph"/>
  <w:LsdException Locked="false" Priority="29" SemiHidden="false"
   UnhideWhenUsed="false" QFormat="true" Name="Quote"/>
  <w:LsdException Locked="false" Priority="30" SemiHidden="false"
   UnhideWhenUsed="false" QFormat="true" Name="Intense Quote"/>
  <w:LsdException Locked="false" Priority="66" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium List 2 Accent 1"/>
  <w:LsdException Locked="false" Priority="67" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 1 Accent 1"/>
  <w:LsdException Locked="false" Priority="68" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 2 Accent 1"/>
  <w:LsdException Locked="false" Priority="69" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 3 Accent 1"/>
  <w:LsdException Locked="false" Priority="70" SemiHidden="false"
   UnhideWhenUsed="false" Name="Dark List Accent 1"/>
  <w:LsdException Locked="false" Priority="71" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful Shading Accent 1"/>
  <w:LsdException Locked="false" Priority="72" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful List Accent 1"/>
  <w:LsdException Locked="false" Priority="73" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful Grid Accent 1"/>
  <w:LsdException Locked="false" Priority="60" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light Shading Accent 2"/>
  <w:LsdException Locked="false" Priority="61" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light List Accent 2"/>
  <w:LsdException Locked="false" Priority="62" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light Grid Accent 2"/>
  <w:LsdException Locked="false" Priority="63" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Shading 1 Accent 2"/>
  <w:LsdException Locked="false" Priority="64" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Shading 2 Accent 2"/>
  <w:LsdException Locked="false" Priority="65" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium List 1 Accent 2"/>
  <w:LsdException Locked="false" Priority="66" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium List 2 Accent 2"/>
  <w:LsdException Locked="false" Priority="67" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 1 Accent 2"/>
  <w:LsdException Locked="false" Priority="68" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 2 Accent 2"/>
  <w:LsdException Locked="false" Priority="69" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 3 Accent 2"/>
  <w:LsdException Locked="false" Priority="70" SemiHidden="false"
   UnhideWhenUsed="false" Name="Dark List Accent 2"/>
  <w:LsdException Locked="false" Priority="71" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful Shading Accent 2"/>
  <w:LsdException Locked="false" Priority="72" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful List Accent 2"/>
  <w:LsdException Locked="false" Priority="73" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful Grid Accent 2"/>
  <w:LsdException Locked="false" Priority="60" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light Shading Accent 3"/>
  <w:LsdException Locked="false" Priority="61" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light List Accent 3"/>
  <w:LsdException Locked="false" Priority="62" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light Grid Accent 3"/>
  <w:LsdException Locked="false" Priority="63" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Shading 1 Accent 3"/>
  <w:LsdException Locked="false" Priority="64" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Shading 2 Accent 3"/>
  <w:LsdException Locked="false" Priority="65" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium List 1 Accent 3"/>
  <w:LsdException Locked="false" Priority="66" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium List 2 Accent 3"/>
  <w:LsdException Locked="false" Priority="67" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 1 Accent 3"/>
  <w:LsdException Locked="false" Priority="68" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 2 Accent 3"/>
  <w:LsdException Locked="false" Priority="69" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 3 Accent 3"/>
  <w:LsdException Locked="false" Priority="70" SemiHidden="false"
   UnhideWhenUsed="false" Name="Dark List Accent 3"/>
  <w:LsdException Locked="false" Priority="71" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful Shading Accent 3"/>
  <w:LsdException Locked="false" Priority="72" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful List Accent 3"/>
  <w:LsdException Locked="false" Priority="73" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful Grid Accent 3"/>
  <w:LsdException Locked="false" Priority="60" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light Shading Accent 4"/>
  <w:LsdException Locked="false" Priority="61" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light List Accent 4"/>
  <w:LsdException Locked="false" Priority="62" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light Grid Accent 4"/>
  <w:LsdException Locked="false" Priority="63" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Shading 1 Accent 4"/>
  <w:LsdException Locked="false" Priority="64" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Shading 2 Accent 4"/>
  <w:LsdException Locked="false" Priority="65" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium List 1 Accent 4"/>
  <w:LsdException Locked="false" Priority="66" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium List 2 Accent 4"/>
  <w:LsdException Locked="false" Priority="67" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 1 Accent 4"/>
  <w:LsdException Locked="false" Priority="68" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 2 Accent 4"/>
  <w:LsdException Locked="false" Priority="69" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 3 Accent 4"/>
  <w:LsdException Locked="false" Priority="70" SemiHidden="false"
   UnhideWhenUsed="false" Name="Dark List Accent 4"/>
  <w:LsdException Locked="false" Priority="71" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful Shading Accent 4"/>
  <w:LsdException Locked="false" Priority="72" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful List Accent 4"/>
  <w:LsdException Locked="false" Priority="73" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful Grid Accent 4"/>
  <w:LsdException Locked="false" Priority="60" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light Shading Accent 5"/>
  <w:LsdException Locked="false" Priority="61" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light List Accent 5"/>
  <w:LsdException Locked="false" Priority="62" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light Grid Accent 5"/>
  <w:LsdException Locked="false" Priority="63" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Shading 1 Accent 5"/>
  <w:LsdException Locked="false" Priority="64" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Shading 2 Accent 5"/>
  <w:LsdException Locked="false" Priority="65" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium List 1 Accent 5"/>
  <w:LsdException Locked="false" Priority="66" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium List 2 Accent 5"/>
  <w:LsdException Locked="false" Priority="67" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 1 Accent 5"/>
  <w:LsdException Locked="false" Priority="68" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 2 Accent 5"/>
  <w:LsdException Locked="false" Priority="69" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 3 Accent 5"/>
  <w:LsdException Locked="false" Priority="70" SemiHidden="false"
   UnhideWhenUsed="false" Name="Dark List Accent 5"/>
  <w:LsdException Locked="false" Priority="71" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful Shading Accent 5"/>
  <w:LsdException Locked="false" Priority="72" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful List Accent 5"/>
  <w:LsdException Locked="false" Priority="73" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful Grid Accent 5"/>
  <w:LsdException Locked="false" Priority="60" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light Shading Accent 6"/>
  <w:LsdException Locked="false" Priority="61" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light List Accent 6"/>
  <w:LsdException Locked="false" Priority="62" SemiHidden="false"
   UnhideWhenUsed="false" Name="Light Grid Accent 6"/>
  <w:LsdException Locked="false" Priority="63" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Shading 1 Accent 6"/>
  <w:LsdException Locked="false" Priority="64" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Shading 2 Accent 6"/>
  <w:LsdException Locked="false" Priority="65" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium List 1 Accent 6"/>
  <w:LsdException Locked="false" Priority="66" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium List 2 Accent 6"/>
  <w:LsdException Locked="false" Priority="67" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 1 Accent 6"/>
  <w:LsdException Locked="false" Priority="68" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 2 Accent 6"/>
  <w:LsdException Locked="false" Priority="69" SemiHidden="false"
   UnhideWhenUsed="false" Name="Medium Grid 3 Accent 6"/>
  <w:LsdException Locked="false" Priority="70" SemiHidden="false"
   UnhideWhenUsed="false" Name="Dark List Accent 6"/>
  <w:LsdException Locked="false" Priority="71" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful Shading Accent 6"/>
  <w:LsdException Locked="false" Priority="72" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful List Accent 6"/>
  <w:LsdException Locked="false" Priority="73" SemiHidden="false"
   UnhideWhenUsed="false" Name="Colorful Grid Accent 6"/>
  <w:LsdException Locked="false" Priority="19" SemiHidden="false"
   UnhideWhenUsed="false" QFormat="true" Name="Subtle Emphasis"/>
  <w:LsdException Locked="false" Priority="21" SemiHidden="false"
   UnhideWhenUsed="false" QFormat="true" Name="Intense Emphasis"/>
  <w:LsdException Locked="false" Priority="31" SemiHidden="false"
   UnhideWhenUsed="false" QFormat="true" Name="Subtle Reference"/>
  <w:LsdException Locked="false" Priority="32" SemiHidden="false"
   UnhideWhenUsed="false" QFormat="true" Name="Intense Reference"/>
  <w:LsdException Locked="false" Priority="33" SemiHidden="false"
   UnhideWhenUsed="false" QFormat="true" Name="Book Title"/>
  <w:LsdException Locked="false" Priority="37" Name="Bibliography"/>
  <w:LsdException Locked="false" Priority="39" QFormat="true" Name="TOC Heading"/>
 </w:LatentStyles>
</xml><![endif]-->
      <style>
<!--
 /* Font Definitions */
 @font-face
        {font-family:Calibri;
        panose-1:2 15 5 2 2 2 4 3 2 4;
        mso-font-charset:0;
        mso-generic-font-family:swiss;
        mso-font-pitch:variable;
        mso-font-signature:-536870145 1073786111 1 0 415 0;}
 /* Style Definitions */
 p.MsoNormal, li.MsoNormal, div.MsoNormal
        {mso-style-unhide:no;
        mso-style-qformat:yes;
        mso-style-parent:"";
        margin-top:0in;
        margin-right:0in;
        margin-bottom:10.0pt;
        margin-left:0in;
        line-height:115%;
        mso-pagination:widow-orphan;
        font-size:11.0pt;
        font-family:"Calibri","sans-serif";
        mso-fareast-font-family:Calibri;
        mso-bidi-font-family:"Times New Roman";}
span.SpellE
        {mso-style-name:"";
        mso-spl-e:yes;}
.MsoChpDefault
        {mso-style-type:export-only;
        mso-default-props:yes;
        font-family:"Calibri","sans-serif";
        mso-ascii-font-family:Calibri;
        mso-fareast-font-family:Calibri;
        mso-hansi-font-family:Calibri;}
@page WordSection1
        {size:8.5in 11.0in;
        margin:1.0in 1.0in 1.0in 1.0in;
        mso-header-margin:.5in;
        mso-footer-margin:.5in;
        mso-paper-source:0;}
div.WordSection1
        {page:WordSection1;}
-->
</style><!--[if gte mso 10]>
<style>
 /* Style Definitions */
 table.MsoNormalTable
        {mso-style-name:"Table Normal";
        mso-tstyle-rowband-size:0;
        mso-tstyle-colband-size:0;
        mso-style-noshow:yes;
        mso-style-priority:99;
        mso-style-parent:"";
        mso-padding-alt:0in 5.4pt 0in 5.4pt;
        mso-para-margin:0in;
        mso-para-margin-bottom:.0001pt;
        mso-pagination:widow-orphan;
        font-size:10.0pt;
        font-family:"Calibri","sans-serif";}
</style>
<![endif]--><!--[if gte mso 9]><xml>
 <o:shapedefaults v:ext="edit" spidmax="1026"/>
</xml><![endif]--><!--[if gte mso 9]><xml>
 <o:shapelayout v:ext="edit">
  <o:idmap v:ext="edit" data="1"/>
 </o:shapelayout></xml><![endif]-->
      <div class="WordSection1">
        <p class="MsoNormal" style="margin-bottom:0in;margin-bottom:.0001pt"><span style="font-size:12.0pt;line-height:115%;font-family:"Times
            New Roman","serif"">Mac
            Hathaway<o:p></o:p></span></p>
        <p class="MsoNormal" style="margin-bottom:0in;margin-bottom:.0001pt"><span style="font-size:12.0pt;line-height:115%;font-family:"Times
            New Roman","serif"">Senior
            Process and Systems Engineer<o:p></o:p></span></p>
        <p class="MsoNormal" style="margin-bottom:0in;margin-bottom:.0001pt"><span style="font-size:12.0pt;line-height:115%;font-family:"Times
            New Roman","serif"">Harvard
            Center for <span class="SpellE">Nanoscale</span> Systems<o:p></o:p></span></p>
        <p class="MsoNormal" style="margin-bottom:0in;margin-bottom:.0001pt"><span style="font-size:12.0pt;line-height:115%;font-family:"Times
            New Roman","serif"">11
            Oxford St.<o:p></o:p></span></p>
        <p class="MsoNormal" style="margin-bottom:0in;margin-bottom:.0001pt"><span style="font-size:12.0pt;line-height:115%;font-family:"Times
            New Roman","serif"">Cambridge,
            MA<span style="mso-spacerun:yes">  </span>02138<o:p></o:p></span></p>
        <p class="MsoNormal" style="margin-bottom:0in;margin-bottom:.0001pt"><span style="font-size:12.0pt;line-height:115%;font-family:"Times
            New Roman","serif"">617-495-9012<o:p></o:p></span></p>
        <p class="MsoNormal" style="margin-bottom:0in;margin-bottom:.0001pt;line-height:
          normal"><span style="font-size:12.0pt;font-family:"Times
            New Roman","serif""><o:p> </o:p></span></p>
      </div>
    </div>
    <div class="moz-cite-prefix">On 11/17/2022 10:32 AM, Martin, Michael
      wrote:<br>
    </div>
    <blockquote type="cite" cite="mid:BN9PR03MB6170DE28A2B671AE774D935EF2079@BN9PR03MB6170.namprd03.prod.outlook.com">
      
      <style type="text/css" style="display:none;">P {margin-top:0;margin-bottom:0;}</style>
      <div style="font-family: Calibri, Arial, Helvetica, sans-serif;
        font-size: 12pt; color: rgb(0, 0, 0); background-color: rgb(255,
        255, 255);" class="elementToProof">
        Hello, <br>
      </div>
      <div style="font-family: Calibri, Arial, Helvetica, sans-serif;
        font-size: 12pt; color: rgb(0, 0, 0); background-color: rgb(255,
        255, 255);" class="elementToProof ContentPasted0 ContentPasted1">
           We are about to re-wrap our BCl3 line with heat tape and
        insulation and are in need of some advice.   In the past we have
        used the rather expensive silicone constant wattage heaters with
        adjustable power control
        <a href="https://urldefense.proofpoint.com/v2/url?u=https-3A__www.mcmaster.com_heat-2Dtape_constant-2Dwattage-2Dheaters-2Dwith-2Dadjustable-2Dtemperature-2Dcontrol-2Dfor-2Dpipes-2Dand-2Dtubes_&d=DwMFAw&c=WO-RGvefibhHBZq3fL85hQ&r=TEMLD8-VsxCGtcVzmvpT5GFNSczskEKHzW6aYlttmIY&m=KWLJCM6ZhWpx1UvrUBWkHKKjEoGzVZrVKbx1lmT96OCO8boDFL9fPSm9_ykSmZuQ&s=7Db1yjuVUcVyMNWVgF_ViFS0RjFPjkEuD6LZ3iMZYVc&e=" id="LPlnkOWALinkPreview" moz-do-not-send="true">
https://www.mcmaster.com/heat-tape/constant-wattage-heaters-with-adjustable-temperature-control-for-pipes-and-tubes/</a>
        .  The problem we have is that these do not seem to last very
        long before burning out, and as I mentioned are quite expensive.
        Does anyone have a better solution?  Longer lasting and cheaper?
        I should mention that we need only to keep the tubing at maybe
        30C to prevent condensation of the BCl3 vapor. 
        <br>
      </div>
      <div class="_Entity _EType_OWALinkPreview _EId_OWALinkPreview
        _EReadonly_1">
        <div id="LPBorder_GTaHR0cHM6Ly93d3cubWNtYXN0ZXIuY29tL2hlYXQtdGFwZS9jb25zdGFudC13YXR0YWdlLWhlYXRlcnMtd2l0aC1hZGp1c3RhYmxlLXRlbXBlcmF0dXJlLWNvbnRyb2wtZm9yLXBpcGVzLWFuZC10dWJlcy8." class="LPBorder400218" style="width: 100%; margin-top: 16px;
          margin-bottom: 16px; position: relative; max-width: 800px;
          min-width: 424px;">
          <table id="LPContainer400218" role="presentation" style="padding: 12px 36px 12px 12px; width: 100%;
            border-width: 1px; border-style: solid; border-color:
            rgb(200, 200, 200); border-radius: 2px;">
            <tbody>
              <tr style="border-spacing: 0px;" valign="top">
                <td>
                  <div id="LPImageContainer400218" style="position:
                    relative; margin-right: 12px; height: 160px;
                    overflow: hidden;">
                    <a target="_blank" id="LPImageAnchor400218" href="https://urldefense.proofpoint.com/v2/url?u=https-3A__www.mcmaster.com_heat-2Dtape_constant-2Dwattage-2Dheaters-2Dwith-2Dadjustable-2Dtemperature-2Dcontrol-2Dfor-2Dpipes-2Dand-2Dtubes_&d=DwMFAw&c=WO-RGvefibhHBZq3fL85hQ&r=TEMLD8-VsxCGtcVzmvpT5GFNSczskEKHzW6aYlttmIY&m=KWLJCM6ZhWpx1UvrUBWkHKKjEoGzVZrVKbx1lmT96OCO8boDFL9fPSm9_ykSmZuQ&s=7Db1yjuVUcVyMNWVgF_ViFS0RjFPjkEuD6LZ3iMZYVc&e=" moz-do-not-send="true"><img id="LPThumbnailImageId400218" alt="" style="display: block;" src="https://images1.mcmaster.com/init/gfx/favicon/192x192.png?ver=1622796110" moz-do-not-send="true" width="160" height="160"></a></div>
                </td>
                <td style="width: 100%;">
                  <div id="LPTitle400218" style="font-size: 21px;
                    font-weight: 300; margin-right: 8px; font-family:
                    "wf_segoe-ui_light", "Segoe UI
                    Light", "Segoe WP Light", "Segoe
                    UI", "Segoe WP", Tahoma, Arial,
                    sans-serif; margin-bottom: 12px;">
                    <a target="_blank" id="LPUrlAnchor400218" href="https://urldefense.proofpoint.com/v2/url?u=https-3A__www.mcmaster.com_heat-2Dtape_constant-2Dwattage-2Dheaters-2Dwith-2Dadjustable-2Dtemperature-2Dcontrol-2Dfor-2Dpipes-2Dand-2Dtubes_&d=DwMFAw&c=WO-RGvefibhHBZq3fL85hQ&r=TEMLD8-VsxCGtcVzmvpT5GFNSczskEKHzW6aYlttmIY&m=KWLJCM6ZhWpx1UvrUBWkHKKjEoGzVZrVKbx1lmT96OCO8boDFL9fPSm9_ykSmZuQ&s=7Db1yjuVUcVyMNWVgF_ViFS0RjFPjkEuD6LZ3iMZYVc&e=" style="text-decoration: none; color:
                      var(--themePrimary);" moz-do-not-send="true">McMaster-Carr</a></div>
                  <div id="LPDescription400218" style="font-size: 14px;
                    max-height: 100px; color: rgb(102, 102, 102);
                    font-family: "wf_segoe-ui_normal",
                    "Segoe UI", "Segoe WP", Tahoma,
                    Arial, sans-serif; margin-bottom: 12px;
                    margin-right: 8px; overflow: hidden;">
                    McMaster-Carr is the complete source for your plant
                    with over 595&#44;000 products. 98% of products
                    ordered ship from stock and deliver same or next
                    day.</div>
                  <div id="LPMetadata400218" style="font-size: 14px;
                    font-weight: 400; color: rgb(166, 166, 166);
                    font-family: "wf_segoe-ui_normal",
                    "Segoe UI", "Segoe WP", Tahoma,
                    Arial, sans-serif;">
                    <a class="moz-txt-link-abbreviated" href="http://www.mcmaster.com">www.mcmaster.com</a></div>
                </td>
              </tr>
            </tbody>
          </table>
        </div>
      </div>
      <div style="font-family: Calibri, Arial, Helvetica, sans-serif;
        font-size: 12pt; color: rgb(0, 0, 0); background-color: rgb(255,
        255, 255);" class="elementToProof ContentPasted2">
           I was looking at self-regulating heat tapes used to prevent
        pipes from freezing (an interesting technology in its own right)
        but am not sure they operate above room temperature given their
        intended application. 
        <a href="https://urldefense.proofpoint.com/v2/url?u=https-3A__www.thecarycompany.com_temperature-2Dcontrol_heating-2Dcables_self-2Dregulating-2Dcables-3Ftemp-5Fvoltage-3D157510&d=DwMFAw&c=WO-RGvefibhHBZq3fL85hQ&r=TEMLD8-VsxCGtcVzmvpT5GFNSczskEKHzW6aYlttmIY&m=KWLJCM6ZhWpx1UvrUBWkHKKjEoGzVZrVKbx1lmT96OCO8boDFL9fPSm9_ykSmZuQ&s=uVM7vhB8VwmRD9MaZyQcnbKLOAHitY3R6t7KI8u58jM&e=" id="LPlnkOWALinkPreview_1" moz-do-not-send="true">
https://www.thecarycompany.com/temperature-control/heating-cables/self-regulating-cables?temp_voltage=157510</a>
        The nice thing about these is that they evidently last for
        years.
        <br>
      </div>
      <div class="_Entity _EType_OWALinkPreview _EId_OWALinkPreview_1
        _EReadonly_1">
        <div id="LPBorder_GTaHR0cHM6Ly93d3cudGhlY2FyeWNvbXBhbnkuY29tL3RlbXBlcmF0dXJlLWNvbnRyb2wvaGVhdGluZy1jYWJsZXMvc2VsZi1yZWd1bGF0aW5nLWNhYmxlcz90ZW1wX3ZvbHRhZ2U9MTU3NTEw" class="LPBorder401269" style="width: 100%; margin-top: 16px;
          margin-bottom: 16px; position: relative; max-width: 800px;
          min-width: 424px;">
          <table id="LPContainer401269" role="presentation" style="padding: 12px 36px 12px 12px; width: 100%;
            border-width: 1px; border-style: solid; border-color:
            rgb(200, 200, 200); border-radius: 2px;">
            <tbody>
              <tr style="border-spacing: 0px;" valign="top">
                <td>
                  <div id="LPImageContainer401269" style="position:
                    relative; margin-right: 12px; height: 160px;
                    overflow: hidden;">
                    <a target="_blank" id="LPImageAnchor401269" href="https://urldefense.proofpoint.com/v2/url?u=https-3A__www.thecarycompany.com_temperature-2Dcontrol_heating-2Dcables_self-2Dregulating-2Dcables-3Ftemp-5Fvoltage-3D157510&d=DwMFAw&c=WO-RGvefibhHBZq3fL85hQ&r=TEMLD8-VsxCGtcVzmvpT5GFNSczskEKHzW6aYlttmIY&m=KWLJCM6ZhWpx1UvrUBWkHKKjEoGzVZrVKbx1lmT96OCO8boDFL9fPSm9_ykSmZuQ&s=uVM7vhB8VwmRD9MaZyQcnbKLOAHitY3R6t7KI8u58jM&e=" moz-do-not-send="true"><img id="LPThumbnailImageId401269" alt="" style="display: block;" src="https://www.thecarycompany.com/media/logo/default/the-cary-company-logo.png" moz-do-not-send="true" width="160" height="160"></a></div>
                </td>
                <td style="width: 100%;">
                  <div id="LPTitle401269" style="font-size: 21px;
                    font-weight: 300; margin-right: 8px; font-family:
                    "wf_segoe-ui_light", "Segoe UI
                    Light", "Segoe WP Light", "Segoe
                    UI", "Segoe WP", Tahoma, Arial,
                    sans-serif; margin-bottom: 12px;">
                    <a target="_blank" id="LPUrlAnchor401269" href="https://urldefense.proofpoint.com/v2/url?u=https-3A__www.thecarycompany.com_temperature-2Dcontrol_heating-2Dcables_self-2Dregulating-2Dcables-3Ftemp-5Fvoltage-3D157510&d=DwMFAw&c=WO-RGvefibhHBZq3fL85hQ&r=TEMLD8-VsxCGtcVzmvpT5GFNSczskEKHzW6aYlttmIY&m=KWLJCM6ZhWpx1UvrUBWkHKKjEoGzVZrVKbx1lmT96OCO8boDFL9fPSm9_ykSmZuQ&s=uVM7vhB8VwmRD9MaZyQcnbKLOAHitY3R6t7KI8u58jM&e=" style="text-decoration: none; color:
                      var(--themePrimary);" moz-do-not-send="true">Self-Regulating
                      Heating Cables</a></div>
                  <div id="LPDescription401269" style="font-size: 14px;
                    max-height: 100px; color: rgb(102, 102, 102);
                    font-family: "wf_segoe-ui_normal",
                    "Segoe UI", "Segoe WP", Tahoma,
                    Arial, sans-serif; margin-bottom: 12px;
                    margin-right: 8px; overflow: hidden;">
                    Automatically Adjust Your Heat Output With
                    Self-Regulating Cables! Keep your pipes from
                    freezing with our Self-Regulating Heating Cables.
                    The cables automatically adjust heat output based on
                    the surface temperature and can also be great for
                    low-temperature process maintenance. The flexibility
                    of the cables can help you get even the most hard to
                    heat applications. Options thermoplastic and
                    fluropolymer jackets as well as tinned copper braid
                    outside finishes. Whether you need low, medium, or
                    high temperature cables, shop and compare all of our
                    selection to find the best fit for you!</div>
                  <div id="LPMetadata401269" style="font-size: 14px;
                    font-weight: 400; color: rgb(166, 166, 166);
                    font-family: "wf_segoe-ui_normal",
                    "Segoe UI", "Segoe WP", Tahoma,
                    Arial, sans-serif;">
                    <a class="moz-txt-link-abbreviated" href="http://www.thecarycompany.com">www.thecarycompany.com</a></div>
                </td>
              </tr>
            </tbody>
          </table>
        </div>
      </div>
      <div style="font-family: Calibri, Arial, Helvetica, sans-serif;
        font-size: 12pt; color: rgb(0, 0, 0); background-color: rgb(255,
        255, 255);" class="elementToProof">
        Also, do you have any recommendations for insulating tubing in a
        cleanroom environment?
        <br>
      </div>
      <div style="font-family: Calibri, Arial, Helvetica, sans-serif;
        font-size: 12pt; color: rgb(0, 0, 0); background-color: rgb(255,
        255, 255);" class="elementToProof">
        <br>
      </div>
      <div style="font-family: Calibri, Arial, Helvetica, sans-serif;
        font-size: 12pt; color: rgb(0, 0, 0); background-color: rgb(255,
        255, 255);" class="elementToProof">
        Regards, <br>
      </div>
      <div style="font-family: Calibri, Arial, Helvetica, sans-serif;
        font-size: 12pt; color: rgb(0, 0, 0); background-color: rgb(255,
        255, 255);" class="elementToProof">
           Michael <br>
      </div>
      <div class="elementToProof">
        <div style="font-family: Calibri, Arial, Helvetica, sans-serif;
          font-size: 12pt; color: rgb(0, 0, 0);">
          <br>
        </div>
        <div id="Signature">
          <div>
            <div id="divtagdefaultwrapper" dir="ltr" style="font-size:12pt; color:#000000;
              font-family:Calibri,Helvetica,sans-serif">
              <p style="margin-top:0px; margin-bottom:0px; margin-top:0;
                margin-bottom:0">Senior Process Engineer </p>
              <p style="margin-top:0px; margin-bottom:0px; margin-top:0;
                margin-bottom:0">Micro/Nano Technology Center</p>
              <p style="margin-top:0px; margin-bottom:0px; margin-top:0;
                margin-bottom:0"><span>University of Louisville</span><br>
              </p>
              <span style="color:rgb(0,0,0); font-size:11pt;
                font-family:Calibri,sans-serif">(502) 552-1945</span><br>
              <p style="margin-top:0px; margin-bottom:0px; margin-top:0;
                margin-bottom:0">Web page:<a href="https://urldefense.proofpoint.com/v2/url?u=https-3A__louisville.edu_micronanohttps-3A__www.instagram.com_micronanolouisville_&d=DwMFAw&c=WO-RGvefibhHBZq3fL85hQ&r=TEMLD8-VsxCGtcVzmvpT5GFNSczskEKHzW6aYlttmIY&m=KWLJCM6ZhWpx1UvrUBWkHKKjEoGzVZrVKbx1lmT96OCO8boDFL9fPSm9_ykSmZuQ&s=_n3p85D3NIeqxSOLhSYW847_zTHmH51vRCYVZcw-Lfc&e=" class="OWAAutoLink" moz-do-not-send="true">
                  https://louisville.edu/micronano</a></p>
              <p style="margin-top:0px; margin-bottom:0px; margin-top:0;
                margin-bottom:0">Instagram:
                <a href="https://urldefense.proofpoint.com/v2/url?u=https-3A__www.instagram.com_micronanolouisville_&d=DwMFAw&c=WO-RGvefibhHBZq3fL85hQ&r=TEMLD8-VsxCGtcVzmvpT5GFNSczskEKHzW6aYlttmIY&m=KWLJCM6ZhWpx1UvrUBWkHKKjEoGzVZrVKbx1lmT96OCO8boDFL9fPSm9_ykSmZuQ&s=NI53uN3DQHoq76ykQ2rjMQNoQEac48VEYtzAIivm3pI&e=" class="OWAAutoLink" moz-do-not-send="true">https://www.instagram.com/micronanolouisville/</a></p>
              <p style="margin-top:0px; margin-bottom:0px; margin-top:0;
                margin-bottom:0">Facebook
                <a href="https://urldefense.proofpoint.com/v2/url?u=https-3A__www.facebook.com_MNTCUOFL_&d=DwMFAw&c=WO-RGvefibhHBZq3fL85hQ&r=TEMLD8-VsxCGtcVzmvpT5GFNSczskEKHzW6aYlttmIY&m=KWLJCM6ZhWpx1UvrUBWkHKKjEoGzVZrVKbx1lmT96OCO8boDFL9fPSm9_ykSmZuQ&s=mD9FJvjnpp6IwZJQ8jOW9u-SNFSQ5_tXB77LPD_lweA&e=" class="OWAAutoLink" moz-do-not-send="true">https://www.facebook.com/MNTCUOFL/</a></p>
              <div>YouTube: <a href="https://urldefense.proofpoint.com/v2/url?u=https-3A__www.youtube.com_channel_UCGiczmq6wVIBJlM7UEGVW9Q&d=DwMFAw&c=WO-RGvefibhHBZq3fL85hQ&r=TEMLD8-VsxCGtcVzmvpT5GFNSczskEKHzW6aYlttmIY&m=KWLJCM6ZhWpx1UvrUBWkHKKjEoGzVZrVKbx1lmT96OCO8boDFL9fPSm9_ykSmZuQ&s=gTTjVkAB72SOgJ5PrbSHAFD-0xqfQLTC6rIZJfIuTDc&e=" class="OWAAutoLink" moz-do-not-send="true">
https://www.youtube.com/channel/UCGiczmq6wVIBJlM7UEGVW9Q</a></div>
              <b><br>
              </b>
            </div>
          </div>
        </div>
      </div>
      <br>
      <fieldset class="moz-mime-attachment-header"></fieldset>
      <pre class="moz-quote-pre" wrap="">_______________________________________________
labnetwork mailing list
<a class="moz-txt-link-abbreviated" href="mailto:labnetwork@mtl.mit.edu">labnetwork@mtl.mit.edu</a>
<a class="moz-txt-link-freetext" href="https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork">https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork</a>
</pre>
    </blockquote>
    <br>
  </body>
</html>