<div dir="ltr">Hello,<div><br></div><div>We haveĀ an MLA150 from Heidelberg instruments which we've been running for ~5 years. At the last annual PM, we were told by Heidelberg that the stage interferometer laser was approaching its end of life, as the signal is getting weaker. Heidelberg quoted us the cost for a refurbished laser unit, and we were surprised by how expensive it was. I was wondering how owners of other Heidelberg Instruments tools have proceeded in this situation? Does everyone just get the unit directly from Heidelberg, or has anyone attempted any thriftier alternatives such as repairing or replacing themselves?</div><div><br></div><div>The laser unit is a Renishaw RLU10-A3-A3.</div><div><br></div><div>Best,</div><div>-Greg Holloway</div><div>QNFCF: University of Waterloo</div></div>