    <p>We use DES (diethylsilane) as our silicon precursor in our Trion
      PECVD system.   The company we deal with for sensors is asking
      10K$ for a sensor that will need to recalibrated yearly and
      replaced after 2 years.  Quite steep in our opinion.  As our DES
      cylinder spends roughly 95% of the time closed, I'd like to find a
      less expensive option.  For example, even a handheld unit that I
      would only use when DES is in use. <br>