<html xmlns:v="urn:schemas-microsoft-com:vml" xmlns:o="urn:schemas-microsoft-com:office:office" xmlns:w="urn:schemas-microsoft-com:office:word" xmlns:m="http://schemas.microsoft.com/office/2004/12/omml" xmlns="http://www.w3.org/TR/REC-html40">
<head>
<meta http-equiv="Content-Type" content="text/html; charset=iso-8859-1">
<meta name="Generator" content="Microsoft Word 15 (filtered medium)">
<style><!--
/* Font Definitions */
@font-face
{font-family:"Cambria Math";
panose-1:2 4 5 3 5 4 6 3 2 4;}
@font-face
{font-family:Calibri;
panose-1:2 15 5 2 2 2 4 3 2 4;}
/* Style Definitions */
p.MsoNormal, li.MsoNormal, div.MsoNormal
{margin:0in;
font-size:11.0pt;
font-family:"Calibri",sans-serif;
mso-ligatures:standardcontextual;}
span.EmailStyle17
{mso-style-type:personal-compose;
font-family:"Calibri",sans-serif;
color:windowtext;}
.MsoChpDefault
{mso-style-type:export-only;
font-family:"Calibri",sans-serif;}
@page WordSection1
{size:8.5in 11.0in;
margin:1.0in 1.0in 1.0in 1.0in;}
div.WordSection1
{page:WordSection1;}
--></style><!--[if gte mso 9]><xml>
<o:shapedefaults v:ext="edit" spidmax="1026" />
</xml><![endif]--><!--[if gte mso 9]><xml>
<o:shapelayout v:ext="edit">
<o:idmap v:ext="edit" data="1" />
</o:shapelayout></xml><![endif]-->
</head>
<body lang="EN-US" link="#0563C1" vlink="#954F72" style="word-wrap:break-word">
<div class="WordSection1">
<p class="MsoNormal">Dear Labnetwork,<o:p></o:p></p>
<p class="MsoNormal"><o:p> </o:p></p>
<p class="MsoNormal">We have found that exposure of SU-8 on our MLA150 tool (using the 375nm laser) seems to require very high doses. Even thin ~500nm thick films (using SU-8 2000.5) have required doses on the order of 1200mJ/cm<sup>2
</sup>to fully expose. This is 15-20x the recommended dosage from both the datasheet and what we estimate is the exposure dose used on our filtered contact aligners. Thicker films follow the same trend, but not necessarily in a linear fashion (5µm films require
~2000mJ/cm<sup>2</sup>).<o:p></o:p></p>
<p class="MsoNormal"><o:p> </o:p></p>
<p class="MsoNormal">I am sure the bump from 365nm to 375nm plays a role, but the magnitude of the change seems excessive. FWIW, our other negative resists (eg. nLOF2020) seem to expose properly at reasonable doses.<o:p></o:p></p>
<p class="MsoNormal"><o:p> </o:p></p>
<p class="MsoNormal">Has anyone else experienced this? Does anyone have an explanation or any processing suggestions for using SU-8 with an MLA?<o:p></o:p></p>
<p class="MsoNormal"><o:p> </o:p></p>
<p class="MsoNormal">Thanks,<o:p></o:p></p>
<p class="MsoNormal">-Dave<o:p></o:p></p>
<p class="MsoNormal" style="mso-margin-top-alt:auto;mso-margin-bottom-alt:auto;line-height:11.25pt;background:white">
<b><span style="font-size:9.0pt;font-family:"Arial",sans-serif;color:#BA0C2F;background:white;mso-ligatures:none">Dave Hollingshead</span></b><span style="font-size:9.0pt;font-family:"Arial",sans-serif;color:#3F4443;mso-ligatures:none"><br>
Manager, Research Operations<br>
<br>
</span><b><span style="font-size:9.0pt;font-family:"Arial",sans-serif;color:#BA0C2F;mso-ligatures:none">The Ohio State University</span></b><span style="font-size:9.0pt;font-family:"Arial",sans-serif;color:#3F4443;mso-ligatures:none"><br>
Nanotech West Labs<br>
Suite 100, 1381 Kinnear Rd, Columbus, OH 43212<br>
614.292.1355 Office<br>
<span style="background:white"><a href="mailto:hollingshead.19@osu.edu"><span style="color:#0563C1">hollingshead.19@osu.edu</span></a></span> /
<a href="http://nanotech.osu.edu"><span style="color:#BA0C2F;background:white">nanotech.osu.edu</span></a><br>
<br>
Pronouns: he/him/his<o:p></o:p></span></p>
<p class="MsoNormal"><o:p> </o:p></p>