<div dir="auto">Dear Matthias,</div>
<div dir="auto"><br>
</div>
<div dir="auto">I would recommend using a pyrolitic graphite target. The result in far less unwanted fine particulate compared to the standard carbon target. They are significantly more expensive. We buy ours from ACI Alloys.</div>
<div dir="auto"><br>
</div>
<div dir="auto">Regards,</div>
<div dir="auto">Kevin </div>
<div id="mail-editor-reference-message-container" dir="auto"><br>
<hr style="display:inline-block;width:98%">
<div id="divRplyFwdMsg" style="font-size: 11pt;"><strong>From:</strong> labnetwork <labnetwork-bounces@mtl.mit.edu> on behalf of Matthew Moneck <mmoneck@andrew.cmu.edu><br>
<strong>Sent:</strong> Wednesday, July 17, 2024 6:45:32 PM<br>
<strong>To:</strong> Matthias Pleil <mpleil@unm.edu><br>
<strong>Cc:</strong> labnetwork@mtl.mit.edu <labnetwork@mtl.mit.edu><br>
<strong>Subject:</strong> Re: [labnetwork] Carbon Targets in Sputter<br>
</div>
<br>
<div dir="ltr">
<div class="gmail_default" style="color: rgb(11, 83, 148);">Hi Matthias,</div>
<div class="gmail_default" style="color: rgb(11, 83, 148);"><br>
</div>
<div class="gmail_default" style="color: rgb(11, 83, 148);">We have done a lot of carbon sputtering and the only real issue we encounter is particulate.  The sputtered carbon can have poor adhesion.  Therefore, it tends to flake off of shields and other components
 coated during sputtering, ultimately forming fine particulate.  We only allow it in one tool for that reason.  That tool also has very good target isolation and shielding, so the particulate we form stays concentrated mainly to that target area, minimizing
 the risk of cross-contamination.  </div>
<div class="gmail_default" style="color: rgb(11, 83, 148);"><br>
</div>
<div class="gmail_default" style="color: rgb(11, 83, 148);">Best Regards,<br>
<br>
Matt</div>
</div>
<br>
<div class="gmail_quote">
<div dir="ltr" class="gmail_attr">On Wed, Jul 17, 2024 at 8:06 AM Matthias Pleil <<a href="mailto:mpleil@unm.edu">mpleil@unm.edu</a>> wrote:<br>
</div>
<blockquote class="gmail_quote" style="margin:0px 0px 0px 0.8ex; border-left:1px solid rgb(204,204,204); padding-left:1ex">
<div class="msg5243029269300502320">
<div dir="ltr">
<div style="font-family: Arial, Helvetica, sans-serif; font-size: 12pt; color: rgb(0, 0, 0);">
Hello LabNetwork folks,</div>
<div style="font-family: Arial, Helvetica, sans-serif; font-size: 12pt; color: rgb(0, 0, 0);">
<br>
</div>
<div style="font-family: Arial, Helvetica, sans-serif; font-size: 12pt; color: rgb(0, 0, 0);">
I have a user that wishes to use a carbon target in our sputter tool.  I have a couple of questions:</div>
<ol start="1" style="margin-top:0px; margin-bottom:0px">
<li style="font-family: Arial, Helvetica, sans-serif; font-size: 12pt; list-style-type: "1) "; color: rgb(0, 0, 0);">
<div>What, if any, concerns should we have regarding cross-contamination.  We typically use the sputter tool for metals and dielectrics.</div>
</li><li style="font-family: Arial, Helvetica, sans-serif; font-size: 12pt; list-style-type: "2) "; color: rgb(0, 0, 0);">
<div>Any suggestions, lessons learned if you have used such targets in the past.</div>
</li></ol>
<div style="font-family: Arial, Helvetica, sans-serif; font-size: 12pt; color: rgb(0, 0, 0);">
<br>
</div>
<div style="font-family: Arial, Helvetica, sans-serif; font-size: 12pt; color: rgb(0, 0, 0);">
Greatly appreciate any input you can provide.  Thanks!</div>
<div style="font-family: Arial, Helvetica, sans-serif; font-size: 12pt; color: rgb(0, 0, 0);">
<br>
</div>
<div id="m_5243029269300502320Signature" style="">
<div style="font-family: Arial, Helvetica, sans-serif; font-size: 14pt; color: rgb(0, 0, 0);">
<br>
</div>
<div id="m_5243029269300502320divtagdefaultwrapper" dir="ltr" style="font-size: 12pt; font-family: Calibri, Arial, Helvetica, sans-serif, EmojiFont, "Apple Color Emoji", "Segoe UI Emoji", NotoColorEmoji, "Segoe UI Symbol", "Android Emoji", EmojiSymbols; color: rgb(0, 0, 0); background-color: rgb(255, 255, 255);">
<div style="margin:0px; font-family:Arial,Helvetica,sans-serif; font-size:14pt">Kind Regards,
</div>
<div style="margin-right:0px; margin-left:0px; font-family:Calibri,Arial,Helvetica,sans-serif">
<br>
</div>
<div style="text-align: left; margin: 0px; font-family: Arial, Helvetica, sans-serif; font-size: 14pt; background-color: rgb(255, 255, 255);">
Matthias Pleil, Ph.D.</div>
<div style="text-align: left; margin: 0px; font-family: Arial, Helvetica, sans-serif; font-size: 14pt; background-color: rgb(255, 255, 255);">
Director Manufacturing Engineering Program</div>
<div style="text-align: left; margin: 0px; font-family: Arial, Helvetica, sans-serif; font-size: 14pt; background-color: rgb(255, 255, 255);">
<span style="background-color: rgb(255, 255, 255);">UNM MTTC Cleanroom Manager</span></div>
<div style="text-align: left; margin: 0px; font-family: Arial, Helvetica, sans-serif; font-size: 14pt; background-color: rgb(255, 255, 255);">
Research Professor & Senior Lecturer III of Mech. Eng - UNM</div>
<div style="text-align: left; margin: 0px; font-family: Arial, Helvetica, sans-serif; font-size: 14pt; background-color: rgb(255, 255, 255);">
PI - NSF Support Center for Microsystems Education</div>
<div style="text-align: left; margin: 0px; font-family: Arial, Helvetica, sans-serif; font-size: 14pt; background-color: rgb(255, 255, 255);">
<br>
</div>
<div style="margin: 0px; background-color: rgb(255, 255, 255);"></div>
<div style="text-align: left; margin: 0px; font-size: 14pt; color: rgb(0, 0, 0); background-color: rgb(255, 255, 255);">
<span style="font-family:Calibri,Arial,Helvetica,sans-serif"><br>
</span><span style="font-family:Arial,Helvetica,sans-serif"></span></div>
<div style="text-align: left; margin: 0px; font-family: Calibri, Arial, Helvetica, sans-serif; background-color: rgb(255, 255, 255);">
<br>
</div>
<div style="margin-right:0px; margin-left:0px; font-family:Calibri,Arial,Helvetica,sans-serif">
<br>
</div>
</div>
</div>
</div>
_______________________________________________<br>
labnetwork mailing list<br>
<a href="mailto:labnetwork@mtl.mit.edu" target="_blank">labnetwork@mtl.mit.edu</a><br>
<a href="https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork" originalsrc="https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork" shash="NDmhmVqmdY7WIPnlbyq+iMpL4Qd9LYIkghxoGHDU7cCZwoTvBBkHRENZIB2maYsCXA6TDYU62BFmTw1wNZp6e3oPo7T6wuYY8P27s7wOplmFeOEiRnwqBv/hgYfdiyJYKZfoQ3YvzyF0Qrg3gs84NjIFG6J7sBcD1fAYZamnWPY=" rel="noreferrer" target="_blank">https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork</a><br>
</div>
</blockquote>
</div>
<br clear="all">
<div><br>
</div>
<span class="gmail_signature_prefix">-- </span><br>
<div dir="ltr" class="gmail_signature">
<div dir="ltr">
<p class="MsoNormal">--<br>
Matthew T. Moneck, Ph.D<br>
Executive Director, Claire & John Bertucci Nanotechnology Laboratory<br>
Electrical & Computer Engineering | Carnegie Mellon University<br>
5000 Forbes Avenue, Pittsburgh, PA 15213-3890<br>
Phone: 412-268-5430<br>
<a href="http://ece.cmu.edu/" originalsrc="http://ece.cmu.edu/" shash="iMXl6W5EFrirpbrYh7/GwoIc7NY8eN2lNz7An/q8iaibE4D+NJlhMAaMfXoy9pge26wEQSw36c9QWZ3RKMl+Ot22Gx8wqLLVsKnKm2kLXmN0eZ0ALhaeMg3Pqj9y0NBEDRqej7UccDNgo750zYv/UVWqnRQwQMqI2UZBjyAXSU4=" target="_blank">ece.cmu.edu</a>
<br>
<a href="http://nanofab.ece.cmu.edu/" originalsrc="http://nanofab.ece.cmu.edu/" shash="LZZ1Lmq5VNWXJFvyt7+eUJ+/j87tGd4P42VIVXgTuxXmsBLgmy8uO1JUjlXpRaz9M4jtB9Sc0jQP/KvBA3grGNm0+GQ2qDSd9lm/3FyEXxwP91UHVKCyjt8QjzKDdeLyJHzLycOEF3HUH8drTqJYdh7rhE3+GAexwFDXTP+NQmw=" target="_blank">nanofab.ece.cmu.edu</a> </p>
</div>
</div>
<br>
</div>
</body>
</html>