<div dir="auto">Dear Lab network,</div>
<div dir="auto"><br>
</div>
<div dir="auto">I am afraid of using TiCl4 precursor in our fab, we had old Savanah 100 system with foreline trap and vacuum pump.</div>
<div dir="auto"><br>
</div>
<div dir="auto">Main canister box is exhausted and pump outlet also in the exhaust line.</div>
<div dir="auto"><br>
</div>
<div dir="auto">On this circumstances, is it safe to use TiCl4 canister for this system?</div>