<div dir="ltr"><div>Hello All,</div><div><br></div><div>Who are you using to supply XeF2 for your etchers? We have an Xactix e1, and we last got our stuff from Pelchem through Linde, but Linde no longer sells XeF2, and it is not yet clear if Linde will sell direct.<br></div><div><br></div><div>I look forward to your responses.<br clear="all"></div><div><br></div><div>Thank you,<br></div><span class="gmail_signature_prefix">-- </span><br><div dir="ltr" class="gmail_signature" data-smartmail="gmail_signature"><div dir="ltr"><div>Kyle Keenan</div><div><br></div><div>Senior Manager - Laboratory Operations<br></div><div>Quattrone Nanofabrication Facility</div><div>University of Pennsylvania</div><div>P: 215-898-7560</div><div>F: 215-573-4925<br></div></div></div></div>