<div dir="auto">Dan here. I have been following the conversation a bit. Has ion beam depostion been considered as a option for your oxide film requirements? Just curious.</div>
<div dir="auto"><br>
</div>
<div dir="auto">Thanks,</div>
<div dir="auto"><br>
</div>
<div dir="auto">Dan</div>
<div dir="auto"><br>
</div>
<div dir="auto"><br>
</div>
<div><br>
</div>
<div><br>
</div>
<div>-------- Original message --------</div>
<div>From: Youry Borisenkov <yb2471@columbia.edu> </div>
<div>Date: 10/22/25 9:01 PM (GMT-05:00) </div>
<div>To: Gabriel Catalano <gcatalano@stanford.edu> </div>
<div>Cc: labnetwork@mtl.mit.edu </div>
<div>Subject: Re: [labnetwork] Experience with Angstrom E-Beam Evaporators? </div>
<div><br>
</div>
<div>
<div dir="auto">Hi Gabriel,</div>
<div dir="auto">I double the previous referral.</div>
<div dir="auto">We have two Angstrom ebeam tools (one older and one newer system) and they are great. Great tools and great service. </div>
<div dir="auto">I never worked with Kj Lesker tools and we do have two AJAs sputtering systems. So I can’t comment on the e-beam performance. The sputtering tools are pretty sturdy and robust. The service tends to be a bit on the slow side, I think they might
 be bigger company (not sure about that) so it takes time to get the answers. </div>
<div dir="auto">Hope this helps. </div>
<div dir="auto">Youry</div>
<div dir="auto"><br>
</div>
<div><br>
<div class="gmail_quote gmail_quote_container">
<div dir="ltr" class="gmail_attr">On Wed, Oct 22, 2025 at 8:05 PM Trieu Nguyen <<a href="mailto:trieu.nguyen@mail.wvu.edu">trieu.nguyen@mail.wvu.edu</a>> wrote:<br>
</div>
<blockquote class="gmail_quote" style="margin:0px 0px 0px 0.8ex; border-left-width:1px; border-left-style:solid; padding-left:1ex; border-left-color:rgb(204,204,204)">
<div style="font-size:1px; line-height:1px; height:0px; max-height:0px; opacity:0; overflow:hidden; display:none!important; color:rgb(255,255,255)">
Hi Gabe, Angstrom is a very good choice for PVD. They have provided very good service and have been highly responsive, replying to emails promptly and even offering free retraining when needed. Best regards, Trieu Nguyen, PhD Cleanroom(s) manager</div>
<div style="font-size:1px; line-height:1px; max-height:0px; opacity:0; overflow:hidden; display:none!important; color:rgb(255,255,255)">
ZjQcmQRYFpfptBannerStart</div>
<u></u>
<div dir="ltr" lang="en" id="m_-9213807626359753855pfptBannercxv3scd" style="display:block!important; text-align:left!important; margin:16px 0px!important; padding:8px 16px!important; border-radius:4px!important; min-width:200px!important; border-top-width:4px!important; border-top-style:solid!important; background-color:rgb(208,216,220); border-top-color:rgb(144,164,174)">
<div id="m_-9213807626359753855pfptBannercxv3scd" style="float:left!important; display:block!important; margin:0px 0px 1px!important; max-width:600px!important">
<div id="m_-9213807626359753855pfptBannercxv3scd" style="font-family:Arial,sans-serif; display:block!important; font-weight:bold!important; font-size:14px!important; line-height:18px!important; background-color:rgb(208,216,220); color:rgb(0,0,0)">
This Message Is From an External Sender </div>
<div id="m_-9213807626359753855pfptBannercxv3scd" style="font-weight:normal; font-family:Arial,sans-serif; display:block!important; font-size:12px!important; line-height:18px!important; margin-top:2px!important; background-color:rgb(208,216,220); color:rgb(0,0,0)">
This message came from outside your organization. </div>
</div>
<div style="height:0px; clear:both!important; display:block!important; line-height:0!important; font-size:0.01px!important">
 </div>
</div>
<u></u>
<div style="font-size:1px; line-height:1px; max-height:0px; opacity:0; overflow:hidden; display:none!important; color:rgb(255,255,255)">
ZjQcmQRYFpfptBannerEnd</div>
<div lang="EN-US" style="">
<div class="m_-9213807626359753855WordSection1">
<p class="MsoNormal"><span style="font-family:Aptos,sans-serif">Hi Gabe,<u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
<p class="MsoNormal"><span style="font-family:Aptos,sans-serif"><u style="font-family:Aptos,sans-serif"></u> <u style="font-family:Aptos,sans-serif"></u></span></p>
<p class="MsoNormal"><span style="font-family:Aptos,sans-serif">Angstrom is a very good choice for PVD. They have provided very good service and have been highly responsive, replying to emails promptly and even offering free retraining when needed.<u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
<p class="MsoNormal"><span style="font-family:Aptos,sans-serif"><u style="font-family:Aptos,sans-serif"></u> <u style="font-family:Aptos,sans-serif"></u></span></p>
<p class="MsoNormal"><span style="font-family:Aptos,sans-serif">Best regards,<u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
<p class="MsoNormal"><span style="font-family:Aptos,sans-serif"><u style="font-family:Aptos,sans-serif"></u> <u style="font-family:Aptos,sans-serif"></u></span></p>
<div>
<p class="MsoNormal"><span style="font-size:12pt; font-family:Aptos,sans-serif; color:rgb(0,112,192)">Trieu Nguyen, PhD</span><span style="font-family:Aptos,sans-serif; color:rgb(0,112,192)"><u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
<p class="MsoNormal"><span style="font-size:12pt; font-family:Aptos,sans-serif; color:rgb(0,112,192)">Cleanroom(s) manager<u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
<p class="MsoNormal"><span style="font-size:12pt; font-family:Aptos,sans-serif; color:rgb(0,112,192)">Shared Research Facilities<u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
<p class="MsoNormal"><span style="font-size:12pt; font-family:Aptos,sans-serif; color:rgb(0,112,192)">West Virginia University<u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
<p class="MsoNormal"><span style="font-size:12pt; font-family:Aptos,sans-serif; color:rgb(0,112,192)">Office: WH 405 | ESB G60<u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
<p class="MsoNormal"><span style="font-size:12pt; font-family:Aptos,sans-serif; color:rgb(0,112,192)">Email:
<a href="mailto:trieu.nguyen@mail.wvu.edu" target="_blank" style="font-family:Aptos,sans-serif">
<span style="font-family:Aptos,sans-serif; color:rgb(0,112,192)">trieu.nguyen@mail.wvu.edu</span></a><u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
<p class="MsoNormal"><span style="font-size:12pt; font-family:Aptos,sans-serif; color:rgb(0,112,192)">Google Scholar:
<a href="https://urldefense.com/v3/__https://scholar.google.com/citations?user=SuHeFCAAAAAJ&hl=en__;!!BDUfV1Et5lrpZQ!UP_tn9x3KYyg5itoeWiYYePgZm5c53OmiGFVCCCQj_NTPOXNfiSZ8F-XaS6CGxjP1N_GuOM0KanGWYEA39JRkRGMaTDsAq7FRg$" target="_blank" style="font-family:Aptos,sans-serif">
<span style="font-family:Aptos,sans-serif; color:rgb(70,120,134)">https://scholar.google.com/citations?user=SuHeFCAAAAAJ&hl=en</span></a><u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
<p class="MsoNormal"><span style="font-size:12pt; font-family:Aptos,sans-serif; color:rgb(0,112,192)">C: 916 532 4710<u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
<p class="MsoNormal"><span style="font-size:12pt; font-family:Aptos,sans-serif; color:rgb(0,112,192)">O: 304 293 5847<u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
</div>
</div>
</div>
<div lang="EN-US" style="">
<div class="m_-9213807626359753855WordSection1">
<p class="MsoNormal"><span style="font-family:Aptos,sans-serif"><u style="font-family:Aptos,sans-serif"></u> <u style="font-family:Aptos,sans-serif"></u></span></p>
<div>
<div style="border-width:1pt medium medium; border-style:solid none none; padding:3pt 0in 0in; border-color:rgb(225,225,225) currentcolor currentcolor">
<p class="MsoNormal"><b>From:</b> labnetwork <<a href="mailto:labnetwork-bounces@mtl.mit.edu" target="_blank">labnetwork-bounces@mtl.mit.edu</a>>
<b>On Behalf Of </b>Peter Lomax<br>
<b>Sent:</b> Wednesday, October 22, 2025 8:20 AM<br>
<b>To:</b> Nathan Fitzpatrick <<a href="mailto:nnelsonfitzpatrick@uwaterloo.ca" target="_blank">nnelsonfitzpatrick@uwaterloo.ca</a>>; Gabriel Catalano <<a href="mailto:gcatalano@stanford.edu" target="_blank">gcatalano@stanford.edu</a>>;
<a href="mailto:labnetwork@mtl.mit.edu" target="_blank">labnetwork@mtl.mit.edu</a><br>
<b>Subject:</b> Re: [labnetwork] Experience with Angstrom E-Beam Evaporators?<u></u><u></u></p>
</div>
</div>
<p class="MsoNormal"><u></u> <u></u></p>
<p class="MsoNormal"><span lang="EN-GB">Hi Gabe,<u></u><u></u></span></p>
<p class="MsoNormal"><span lang="EN-GB"><u></u> <u></u></span></p>
<p class="MsoNormal"><span lang="EN-GB">We have both a sputter and e-beam evaporator.  We’ve been really impressed with both the equipment and the service – despite us being in Scotland.<u></u><u></u></span></p>
<p class="MsoNormal"><span lang="EN-GB"><u></u> <u></u></span></p>
<p class="MsoNormal"><span lang="EN-GB">The equipment is very easy to use with similar software.<u></u><u></u></span></p>
<p class="MsoNormal"><span lang="EN-GB"><u></u> <u></u></span></p>
<p class="MsoNormal"><span lang="EN-GB">Best<u></u><u></u></span></p>
<p class="MsoNormal"><span lang="EN-GB"><u></u> <u></u></span></p>
<p class="MsoNormal"><span lang="EN-GB">Peter<u></u><u></u></span></p>
<p class="MsoNormal"><span lang="EN-GB"><u></u> <u></u></span></p>
<div>
<div style="border-width:1pt medium medium; border-style:solid none none; padding:3pt 0in 0in; border-color:rgb(225,225,225) currentcolor currentcolor">
<p class="MsoNormal"><b>From:</b> labnetwork <<a href="mailto:labnetwork-bounces@mtl.mit.edu" target="_blank">labnetwork-bounces@mtl.mit.edu</a>>
<b>On Behalf Of </b>Nathan Fitzpatrick<br>
<b>Sent:</b> 21 October 2025 22:28<br>
<b>To:</b> Gabriel Catalano <<a href="mailto:gcatalano@stanford.edu" target="_blank">gcatalano@stanford.edu</a>>;
<a href="mailto:labnetwork@mtl.mit.edu" target="_blank">labnetwork@mtl.mit.edu</a><br>
<b>Subject:</b> Re: [labnetwork] Experience with Angstrom E-Beam Evaporators?<u></u><u></u></p>
</div>
</div>
<p class="MsoNormal"><span lang="EN-GB"><u></u> <u></u></span></p>
<table border="0" cellspacing="0" cellpadding="0" align="left" width="100%" style="width:100%">
<tbody>
<tr>
<td style="background:repeat rgb(166,166,166); padding:0in"></td>
<td width="100%" style="background-image:revert!important; background-position:revert!important; background-size:revert!important; background-repeat:revert!important; background-origin:revert!important; background-clip:revert!important; border-width:revert!important; border-style:revert!important; direction:revert!important; display:revert!important; font-size:revert!important; height:revert!important; letter-spacing:revert!important; line-height:revert!important; margin:revert!important; opacity:revert!important; outline:revert!important; overflow:revert!important; padding:revert!important; table-layout:revert!important; text-align:revert!important; text-indent:revert!important; text-orientation:revert!important; text-overflow:revert!important; text-transform:revert!important; vertical-align:revert!important; white-space:revert!important; width:revert!important; word-break:revert!important; word-spacing:revert!important; writing-mode:revert!important; zoom:revert!important; background-color:revert; border-color:revert; color:revert">
<div>
<p class="MsoNormal"><span style="color:black">You don't often get email from <a href="mailto:nnelsonfitzpatrick@uwaterloo.ca" target="_blank">
nnelsonfitzpatrick@uwaterloo.ca</a>. <a href="https://urldefense.com/v3/__https://aka.ms/LearnAboutSenderIdentification__;!!BDUfV1Et5lrpZQ!UP_tn9x3KYyg5itoeWiYYePgZm5c53OmiGFVCCCQj_NTPOXNfiSZ8F-XaS6CGxjP1N_GuOM0KanGWYEA39JRkRGMaTAB9uXNBQ$" target="_blank">
Learn why this is important</a> </span><u></u><u></u></p>
</div>
</td>
<td style="background-image:revert!important; background-position:revert!important; background-size:revert!important; background-repeat:revert!important; background-origin:revert!important; background-clip:revert!important; border-width:revert!important; border-style:revert!important; direction:revert!important; display:revert!important; font-size:revert!important; height:revert!important; letter-spacing:revert!important; line-height:revert!important; margin:revert!important; opacity:revert!important; outline:revert!important; overflow:revert!important; padding:revert!important; table-layout:revert!important; text-align:revert!important; text-indent:revert!important; text-orientation:revert!important; text-overflow:revert!important; text-transform:revert!important; vertical-align:revert!important; white-space:revert!important; width:revert!important; word-break:revert!important; word-spacing:revert!important; writing-mode:revert!important; zoom:revert!important; background-color:revert; border-color:revert; color:revert">
</td>
</tr>
</tbody>
</table>
<div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif; color:black">Hi Gabe,<u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif; color:black"><u style="font-family:Aptos,sans-serif"></u> <u style="font-family:Aptos,sans-serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif; color:black">Angstrom is a very good choice for PVD hardware.  Our lab has 4 Angstrom systems (1 E-beam, 2 Thermal, 1 LPCVD) and we are quite happy with our purchases.
  They have been a very good partner for our lab.  We also benefit greatly by having local support since Angstrom is 30 minutes away from my office.<u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif; color:black"><u style="font-family:Aptos,sans-serif"></u> <u style="font-family:Aptos,sans-serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif; color:black">Nothing in the equipment world is perfect, but I would be happy to talk openly (offline) about Angstrom’s strengths and weaknesses.  I’m somewhat to very
 familiar with the offerings from the other vendors on your list as well.  I think everyone you are looking at is good.<u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif; color:black"><u style="font-family:Aptos,sans-serif"></u> <u style="font-family:Aptos,sans-serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif; color:black">Best,<u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif; color:black">  -Nathan<u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif; color:black"><u style="font-family:Aptos,sans-serif"></u> <u style="font-family:Aptos,sans-serif"></u></span></p>
</div>
<div id="m_-9213807626359753855ms-outlook-mobile-signature">
<p style="margin:0in"><span lang="EN-GB" style="font-size:13.5pt; font-family:"Times New Roman",serif">-- </span><span lang="EN-GB"><u></u><u></u></span></p>
<p style="margin:0in"><span lang="EN-GB" style="font-size:10pt; font-family:Verdana,sans-serif; color:black">Nathan Fitzpatrick  PhD, PEng   (He/Him)</span><span lang="EN-GB"><u></u><u></u></span></p>
<p style="margin:0in"><span lang="EN-GB" style="font-size:10pt; font-family:Verdana,sans-serif; color:black">Director, Quantum-Nano Fabrication and Characterization Facility (QNFCF)</span><span lang="EN-GB"><u></u><u></u></span></p>
<p style="margin:0in"><span lang="EN-GB" style="font-size:10pt; font-family:Verdana,sans-serif; color:black">Office of Research</span><span lang="EN-GB"><u></u><u></u></span></p>
<p style="margin:0in"><span lang="EN-GB" style="font-size:10pt; font-family:Verdana,sans-serif; color:black">University of Waterloo</span><span lang="EN-GB"><u></u><u></u></span></p>
<p style="margin:0in"><span lang="EN-GB" style="font-size:10pt; font-family:Verdana,sans-serif; color:black"><a href="https://www.google.com/maps/search/200+University+Avenue+West,+Waterloo,+ON++N2L+3G1?entry=gmail&source=g" style="font-family:Verdana,sans-serif">200
 University Avenue West,</a> <a href="https://www.google.com/maps/search/200+University+Avenue+West,+Waterloo,+ON++N2L+3G1?entry=gmail&source=g" style="font-family:Verdana,sans-serif">Waterloo, ON
</a> <a href="https://www.google.com/maps/search/200+University+Avenue+West,+Waterloo,+ON++N2L+3G1?entry=gmail&source=g" style="font-family:Verdana,sans-serif">N2L 3G1</a></span><span lang="EN-GB"><u></u><u></u></span></p>
<p style="margin:0in"><span lang="EN-GB" style="font-size:10pt; font-family:Verdana,sans-serif; color:black">P: 519-888-4567 ext. 31796</span><span lang="EN-GB"><u></u><u></u></span></p>
<p style="margin:0in"><span lang="EN-GB" style="font-size:10pt; font-family:Verdana,sans-serif; color:black">C: 226-218-3206</span><span lang="EN-GB"><u></u><u></u></span></p>
<p style="margin:0in"><u><span lang="EN-GB" style="font-size:10pt; font-family:Verdana,sans-serif; color:rgb(5,99,193)"><a href="https://urldefense.com/v3/__https://uwaterloo.ca/quantum-nano-fabrication-and-characterization-facility/__;!!BDUfV1Et5lrpZQ!UP_tn9x3KYyg5itoeWiYYePgZm5c53OmiGFVCCCQj_NTPOXNfiSZ8F-XaS6CGxjP1N_GuOM0KanGWYEA39JRkRGMaTBljFbUDw$" target="_blank" style="font-family:Verdana,sans-serif"><span style="font-family:Verdana,sans-serif; color:rgb(5,99,193)">https://uwaterloo.ca/qnfcf/</span></a></span></u><span lang="EN-GB"><u></u><u></u></span></p>
<p style="margin:0in"><span lang="EN-GB" style="font-family:"Times New Roman",serif; color:black"> </span><span lang="EN-GB"><u></u><u></u></span></p>
<p style="margin:0in"><span lang="EN-GB" style="font-family:"Times New Roman",serif"><img border="0" src="cid:ii_19a0e66eeb1ad7999131" style="width:319px; max-width:100%"></span><span lang="EN-GB"><u></u><u></u></span></p>
</div>
<div id="m_-9213807626359753855mail-editor-reference-message-container">
<div style="border-width:1pt medium medium; border-style:solid none none; padding:3pt 0in 0in; border-color:currentcolor">
<p class="MsoNormal" style="margin-bottom:12pt"><b><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif; color:black">From:
</span></b><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif; color:black">labnetwork <<a href="mailto:labnetwork-bounces@mtl.mit.edu" target="_blank" style="font-family:Aptos,sans-serif">labnetwork-bounces@mtl.mit.edu</a>> on behalf of
 Gabriel Catalano <<a href="mailto:gcatalano@stanford.edu" target="_blank" style="font-family:Aptos,sans-serif">gcatalano@stanford.edu</a>><br>
<b style="font-family:Aptos,sans-serif">Date: </b>Monday, October 20, 2025 at 9:31</span><span lang="EN-GB" style="font-size:12pt; font-family:Arial,sans-serif; color:black"> </span><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif; color:black">PM<br>
<b style="font-family:Aptos,sans-serif">To: </b><a href="mailto:labnetwork@mtl.mit.edu" target="_blank" style="font-family:Aptos,sans-serif">labnetwork@mtl.mit.edu</a> <<a href="mailto:labnetwork@mtl.mit.edu" target="_blank" style="font-family:Aptos,sans-serif">labnetwork@mtl.mit.edu</a>><br>
<b style="font-family:Aptos,sans-serif">Subject: </b>[labnetwork] Experience with Angstrom E-Beam Evaporators?<u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif; color:black">Hello All, <u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif; color:black"><u style="font-family:Aptos,sans-serif"></u> <u style="font-family:Aptos,sans-serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif; color:black">We are in the process of procuring a new E-Beam evaporator and considering options from Kurt J. Lesker, AJA Internation, and Angstrom Engineering; the
 pricing between all three vendors is comparable. We have lots experience using and maintaining KJL and AJA systems, but do not have much exposure to Angstrom Engineering's systems. We are curious for other nanolabs experience with these tools, particularly
 from a maintenance prospective. We plan to use this tool for both metal and oxide depositions. Any feedback or thoughts on Angstrom's E-beam systems is very much appreciated! <u style="font-family:Aptos,sans-serif"></u><u style="font-family:Aptos,sans-serif"></u></span></p>
</div>
<div id="m_-9213807626359753855Signature">
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif; color:black"><u style="font-family:Aptos,sans-serif"></u> <u style="font-family:Aptos,sans-serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; color:black">Kind Regards,<u></u><u></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; color:black">------------------------<u></u><u></u></span></p>
</div>
<div>
<p class="MsoNormal"><b><span lang="EN-GB" style="font-size:12pt; font-family:"Times New Roman",serif; color:black">Gabe Catalano</span></b><span lang="EN-GB" style="font-size:12pt; font-family:"Times New Roman",serif; color:black"><u style="font-family:"Times New Roman",serif"></u><u style="font-family:"Times New Roman",serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:"Times New Roman",serif; color:black">Lab Operations<u style="font-family:"Times New Roman",serif"></u><u style="font-family:"Times New Roman",serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:"Times New Roman",serif; color:black">Stanford Nanofabrication Facility (SNF)<u style="font-family:"Times New Roman",serif"></u><u style="font-family:"Times New Roman",serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:"Times New Roman",serif; color:black">(650) 498-4014<u style="font-family:"Times New Roman",serif"></u><u style="font-family:"Times New Roman",serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:"Times New Roman",serif; color:black"><a href="https://urldefense.com/v3/__https://snf.stanford.edu/__;!!BDUfV1Et5lrpZQ!UP_tn9x3KYyg5itoeWiYYePgZm5c53OmiGFVCCCQj_NTPOXNfiSZ8F-XaS6CGxjP1N_GuOM0KanGWYEA39JRkRGMaTBeG8Sh3Q$" target="_blank" style="font-family:"Times New Roman",serif">https://snf.stanford.edu/</a><u style="font-family:"Times New Roman",serif"></u><u style="font-family:"Times New Roman",serif"></u></span></p>
</div>
<div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; color:black"><u></u> <u></u></span></p>
</div>
</div>
</div>
</div>
<p class="MsoNormal"><span lang="EN-GB" style="font-size:12pt; font-family:Aptos,sans-serif">The University of Edinburgh is a charitable body, registered in Scotland, with registration number SC005336. Is e buidheann carthannais a th’ ann an Oilthigh Dhùn Èideann,
 clàraichte an Alba, àireamh clàraidh SC005336. <u style="font-family:Aptos,sans-serif">
</u><u style="font-family:Aptos,sans-serif"></u></span></p>
</div>
</div>
<div lang="EN-US" style="">
<div class="m_-9213807626359753855WordSection1"></div>
</div>
_______________________________________________<br>
labnetwork mailing list<br>
<a href="mailto:labnetwork@mtl.mit.edu" target="_blank">labnetwork@mtl.mit.edu</a><br>
<a href="https://urldefense.com/v3/__https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork__;!!BDUfV1Et5lrpZQ!UP_tn9x3KYyg5itoeWiYYePgZm5c53OmiGFVCCCQj_NTPOXNfiSZ8F-XaS6CGxjP1N_GuOM0KanGWYEA39JRkRGMaTBN8h8Xrw$" rel="noreferrer" target="_blank">https://urldefense.com/v3/__https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork__;!!BDUfV1Et5lrpZQ!UP_tn9x3KYyg5itoeWiYYePgZm5c53OmiGFVCCCQj_NTPOXNfiSZ8F-XaS6CGxjP1N_GuOM0KanGWYEA39JRkRGMaTBN8h8Xrw$</a>
<br>
</blockquote>
</div>
</div>
</div>
</body>
</html>