<p>Dear Labnetwork,</p>
<p>As many labs do, because of safety concerns for the students, I
banned the use the real pirahna etch in favor of Purestrip
(Transene version of nanostrip). The problem I have is that the
solution eventually leaks from the bottle. I have heard of others
mentioning this also. </p>
<p>I am now thinking of revising this policy and going back to old
pirahna, despite the issues with safety and aging H2O2.</p>
<p>Anyone have comments?</p>
<p>Mario</p>