<!DOCTYPE html>
<html>
  <head>
    <meta http-equiv="Content-Type" content="text/html; charset=UTF-8">
  </head>
  <body>
    <p>Shimon,</p>
    <p><br>
    </p>
    <p>Demis will be able to help you. I'm attaching a link to our
      Nanofab. The rates are very reasonable.</p>
    <p><br>
    </p>
    <p><a class="moz-txt-link-freetext" href="https://nanofab.ucsb.edu/">https://nanofab.ucsb.edu/</a></p>
    <p><a class="moz-txt-link-freetext" href="https://nanofab.ucsb.edu/services">https://nanofab.ucsb.edu/services</a></p>
    <p><br>
    </p>
    <p>Prashant</p>
    <p>CC: Demis</p>
    <p><br>
    </p>
    <div class="moz-cite-prefix">On 1/31/2026 9:54 AM, Shimon Eliav
      wrote:<br>
    </div>
    <blockquote type="cite"
cite="mid:PR3PR10MB4030B4ACE93908C0D1557345D69CA@PR3PR10MB4030.EURPRD10.PROD.OUTLOOK.COM">
      <meta http-equiv="Content-Type" content="text/html; charset=UTF-8">
      <style type="text/css" style="display:none;"> P {margin-top:0;margin-bottom:0;} </style>
      <div
style="font-family: Aptos, Aptos_EmbeddedFont, Aptos_MSFontService, Calibri, Helvetica, sans-serif; font-size: 11pt; color: rgb(0, 0, 0);"
        class="elementToProof">
        Hello,</div>
      <div
style="font-family: Aptos, Aptos_EmbeddedFont, Aptos_MSFontService, Calibri, Helvetica, sans-serif; font-size: 11pt; color: rgb(0, 0, 0);"
        class="elementToProof">
        An Israeli start-up company is looking for a fab with stepper
        capabilities.</div>
      <div
style="font-family: Aptos, Aptos_EmbeddedFont, Aptos_MSFontService, Calibri, Helvetica, sans-serif; font-size: 11pt; color: rgb(0, 0, 0);"
        class="elementToProof">
        Their process is quite simple: Metal deposition, lithography
        with 1 micron resolution, etching and dicing. Substrate: Si 8".</div>
      <div
style="font-family: Aptos, Aptos_EmbeddedFont, Aptos_MSFontService, Calibri, Helvetica, sans-serif; font-size: 11pt; color: rgb(0, 0, 0);"
        class="elementToProof">
        Regards,</div>
      <div
style="font-family: Aptos, Aptos_EmbeddedFont, Aptos_MSFontService, Calibri, Helvetica, sans-serif; font-size: 11pt; color: rgb(0, 0, 0);"
        class="elementToProof">
        Shimon</div>
      <div><br>
      </div>
      <br>
      <fieldset class="moz-mime-attachment-header"></fieldset>
      <pre wrap="" class="moz-quote-pre">_______________________________________________
labnetwork mailing list
<a class="moz-txt-link-abbreviated" href="mailto:labnetwork@mtl.mit.edu">labnetwork@mtl.mit.edu</a>
<a class="moz-txt-link-freetext" href="https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork">https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork</a>
</pre>
    </blockquote>
    <pre class="moz-signature" cols="72">-- 
Prashant Srinivasan,
Teaching Cleanroom Manager
Department of Electrical and Computer Engineering
University of California Santa Barbara
Santa Barbara, CA 93106
<a class="moz-txt-link-freetext" href="https://www.ece.ucsb.edu/department-resources/electronics-shop/tcr">https://www.ece.ucsb.edu/department-resources/electronics-shop/tcr</a></pre>
  </body>
</html>