    <p>Dear Network,</p>
    <p>We have inherited an old XPS machine.  The XPS part works fine
      and we know how to acquire data.  For analysis, we will certainly
      consult experts before publishing as we are aware of the potential
      pitfalls.  </p>
    <p>We also have an Argon source and sputter power supply and we
      would like to sputter our sample surfaces to remove surface
      contaminants.  The problem: we are neophytes at that part of the
      process besides operating the cylinder and leak valve.</p>
    <p>My question: What are the typical Ar pressures and power settings
      generally used for sputtering?</p>
    <p>Please respond privately or through the network.</p>
    <p>Big THANK YOU.</p>