<div dir="auto">I've seen that in our lam 9600 for years. My suspicion is that it's boron oxide or nitride as a byproduct of the BCl3 reactions. A wet clean should suffice, but SF6/O2 should also mitigate it. (BF3 is volatile, and F can slowly break the B-O and B-N bonds.)<div dir="auto"><br></div><div dir="auto">I would check your chamber and gas panel leak up rates if you are getting a lot of formation rapidly, because an atmosphere leak will generate this stuff much faster. But it's going to form even if your system is sealed tight, especially if you start etching metal oxides on purpose.</div><div dir="auto"><br></div><div dir="auto">Theoretically adding a diluent gas should help but I've never needed to try that hard to mitigate it as long as we keep up with cleaning.</div><div dir="auto"><br></div><div dir="auto">You should assume the substance has unreacted B-Cl in its matrix and generally proceed with the appropriate caution for handling a material that can volatilize chlorine in very small quantities. We stick an exhaust snorkel over the chamber and let it absorb water from the air for quite a while before working on it. It'll pull moisture from the air and offgas HCl.</div></div><br><div class="gmail_quote gmail_quote_container"><div dir="ltr" class="gmail_attr">On Tue, Jun 9, 2026, 5:04 PM Emma Anquillare <<a href="mailto:eanquillare@gc.cuny.edu">eanquillare@gc.cuny.edu</a>> wrote:<br></div><blockquote class="gmail_quote" style="margin:0 0 0 .8ex;border-left:1px #ccc solid;padding-left:1ex">
<div dir="ltr">
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0)">
Dear LabNetwork Hive Mind, </div>
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0)">
<br>
</div>
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0)">
I went to manually scrub out our ICP-Cl Etcher with IPA as I usually do every 1-2 weeks, and opened up the chamber to find large quantities of white powder caked along the upper portion of the metal rim near where it meets the ceramic liner. Large amounts
of it seemed to have fallen onto the table as well. (See Photos). Has anyone ever encountered this? Any idea what it might be?</div>
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0)">
<br>
</div>
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0)">
Here are my suspicions and more details: </div>
<ol start="1" style="margin-top:0px;margin-bottom:0px">
<li style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0);margin-top:0px;margin-bottom:0px;list-style-type:"1) "">
<div role="presentation">One of my colleagues commented that it looked like the Aluminum/a she gets in her deposition tools, and I was wondering if something is leeching out of the liner and it needs to be replaced? Might explain why
it's concentrated at the border, and appears in such visibly large quantities for a nano-scale etch tool</div>
</li><li style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0);margin-top:0px;margin-bottom:0px;list-style-type:"2) "">
<div role="presentation">The immediate suspect of course is also a solid etch product, but we have not had any new or unusual materials in the chamber since the last cleaning two weeks ago (or at least, as far as users have told us).
We have recently changed our clean recipes so that instead of just a blanket O2 clean for everything, there are now customized cleans based on what people are etching, but people seem to be following the rules on this pretty well (see attached). I have also
attached a summary of what has been etched in the chamber since the last manual clean and using what gasses. (We are aware LiNbO3 is not volatile, thus the regular manual cleanings). One thing that also occurred to me was the possibility of LiF formation
with increasing amounts of CF4 being run from the new cleans and reacting with sputtered LiNbO3 in the chamber (but again, this seems like an uncannily large quantity of solid for that). </div>
</li></ol>
<div style="margin-top:0px;margin-bottom:0px;font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0)">
<br>
</div>
<div style="margin-top:0px;margin-bottom:0px;font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0)">
I collected some with kapton tape for XPS analysis, but curious to see if anyone else has encountered this, especially if it's an issue with the tool liner itself.</div>
<div style="margin-top:0px;margin-bottom:0px;font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0)">
<br>
</div>
<div style="margin-top:0px;margin-bottom:0px;font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0)">
Thanks!</div>
<div style="margin-top:0px;margin-bottom:0px;font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0)">
Emma</div>
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0)">
<br>
</div>
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0)">
<br>
</div>
<div id="m_-6236991227201099608Signature">
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0)">
<br>
</div>
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0)">
<b>_____________________________________________</b></div>
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0)">
<b>Emma Anquillare, PhD</b></div>
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:12pt;color:rgb(0,0,0)">
Research Scientist</div>
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;color:rgb(0,0,0)">
<span style="font-size:12pt">ASRC </span><span style="font-size:16px;background-color:rgb(255,255,255)">Nanofabrication Facility</span></div>
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:16px;color:rgb(0,0,0)">
<span style="background-color:rgb(255,255,255)">City University of New York</span></div>
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:16px;color:rgb(0,0,0)">
<span style="background-color:rgb(255,255,255)"><br>
</span></div>
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:16px;color:rgb(0,0,0)">
<img id="m_-6236991227201099608image_0" width="337" height="77" style="width:337px;height:77px" src="cid:2f9751bd-2a5f-49de-a534-a7be1365b2b3"></div>
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:16px;color:rgb(0,0,0)">
<i>Catalyzing Change, Celebrating Gains: </i></div>
<div style="font-family:Aptos,Aptos_EmbeddedFont,Aptos_MSFontService,Calibri,Helvetica,sans-serif;font-size:16px;color:rgb(0,0,0)">
<i>A decade of visionary science for the public good.</i></div>
</div>
</div>
_______________________________________________<br>
labnetwork mailing list<br>
<a href="mailto:labnetwork@mtl.mit.edu" target="_blank" rel="noreferrer">labnetwork@mtl.mit.edu</a><br>
<a href="https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork" rel="noreferrer noreferrer" target="_blank">https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork</a><br>
</blockquote></div>