Seconded. Pretty much everyone I know has moved to dischem for EBL purposes.
<div><br>
</div>
<div>-Shane<br id="lineBreakAtBeginningOfSignature">
<div dir="ltr">Sent from my iPhone</div>
<div dir="ltr"><br>
<blockquote type="cite">On Aug 11, 2026, at 5:34 PM, Price, Aimee <price.798@osu.edu> wrote:<br>
<br>
</blockquote>
</div>
<blockquote type="cite">
<div dir="ltr"><!-- BaNnErBlUrFlE-BoDy-start --><!-- Preheader Text : BEGIN -->
<div style="display:none !important;display:none;visibility:hidden;mso-hide:all;font-size:1px;color:#ffffff;line-height:1px;max-height:0px;opacity:0;overflow:hidden;">
Hi Amir, We get ours from Dischem (2%, 4%, 16%, and 20%). They call it HSiQ. The contact is Andy Thompson, andy@ dischem. com. They are in Pittsburgh and mix it on order, but the resin comes from Canada so there is sometimes a tariff fee. He’ll</div>
<!-- Preheader Text : END --><!-- Email Banner : BEGIN -->
<div style="display:none !important;display:none;visibility:hidden;mso-hide:all;font-size:1px;color:#ffffff;line-height:1px;max-height:0px;opacity:0;overflow:hidden;">
ZjQcmQRYFpfptBannerStart</div>
<!--[if ((ie)|(mso))]>
<table border="0" cellspacing="0" cellpadding="0" width="100%" style="padding: 0px 0px 10px 0px; direction: ltr" lang="en"><tr><td>
<table border="0" cellspacing="0" cellpadding="0" style="padding: 0px 8px 6px 8px; width: 100%; border-radius:4px; border-top:4px solid #90a4ae;background-color:#d0d8dc;"><tr><td valign="top">
<table align="left" border="0" cellspacing="0" cellpadding="0" style="padding: 0px 8px 4px 8px; font-size: 12px; line-height: 16px">
<tr><td style="color:#000000; font-family: 'Arial', sans-serif; font-weight:bold; font-size:14px; line-height: 20px; direction: ltr">
This Message Is From an Untrusted Sender
</td></tr>
<tr><td style="color:#000000; font-weight:normal; font-family: 'Arial', sans-serif; font-size:12px; direction: ltr">
You have not previously corresponded with this sender.
</td></tr>
<tr><td style="color:#000000; font-weight:normal; font-family: 'Arial', sans-serif; font-size:12px; direction: ltr">
See https://it.uw.edu/email-tags for additional information. Please contact the UW-IT Service Center, help@uw.edu 206.221.5000, for assistance.
</td></tr>
</table>
</td></tr></table>
</td></tr></table>
<![endif]--><!--[if !((ie)|(mso))]-->
<div dir="ltr" lang="en" id="pfptBannerud867qm" style="all: revert !important; display:block !important; text-align: left !important; margin: 0 0 10px 0 !important; padding:7px 16px 8px 16px !important; border-radius: 4px !important; min-width: 200px !important; background-color: #d0d8dc !important; background-color: #d0d8dc; border-top: 4px solid #90a4ae !important; border-top: 4px solid #90a4ae;">
<div id="pfptBannerud867qm" style="all: unset !important; float:left !important; display:block !important; margin: 1px 0 1px 0 !important; max-width: 600px !important;">
<div id="pfptBannerud867qm" style="all: unset !important; display:block !important; visibility: visible !important; background-color: #d0d8dc !important; color:#000000 !important; color:#000000; font-family: 'Arial', sans-serif !important; font-family: 'Arial', sans-serif; font-weight:bold !important; font-weight:bold; font-size:14px !important; line-height:1.29 !important; line-height:1.29">
This Message Is From an Untrusted Sender </div>
<div id="pfptBannerud867qm" style="all: unset !important; display:block !important; visibility: visible !important; background-color: #d0d8dc !important; color:#000000 !important; color:#000000; font-weight:normal; font-family: 'Arial', sans-serif !important; font-family: 'Arial', sans-serif; font-size:12px !important; line-height:1.5 !important; line-height:1.5; margin-top:2px !important;">
You have not previously corresponded with this sender. </div>
<div id="pfptBannerud867qm" style="all: unset !important; display:block !important; visibility: visible !important; background-color: #d0d8dc !important; color:#000000 !important; color:#000000; font-weight:normal; font-family: 'Arial', sans-serif !important; font-family: 'Arial', sans-serif; font-size:12px !important; line-height:1.5 !important; line-height:1.5; margin-top:2px !important;">
See https://it.uw.edu/email-tags for additional information. Please contact the UW-IT Service Center, help@uw.edu 206.221.5000, for assistance.
</div>
</div>
<div style="clear: both !important; display: block !important; visibility: hidden !important; line-height: 0 !important; font-size: 0.01px !important; height: 0px">
</div>
</div>
<!--[endif]-->
<div style="display:none !important;display:none;visibility:hidden;mso-hide:all;font-size:1px;color:#ffffff;line-height:1px;max-height:0px;opacity:0;overflow:hidden;">
ZjQcmQRYFpfptBannerEnd</div>
<!-- Email Banner : END --><!-- BaNnErBlUrFlE-BoDy-end --><!-- BaNnErBlUrFlE-HeAdEr-start --><style>#pfptBannerud867qm { color-scheme: revert !important; math-depth: revert !important; ruby-position: revert !important; writing-mode: revert !important; font-family: revert !important; font-feature-settings: revert !important; font-kerning: revert !important; font-optical-sizing: revert !important; font-palette: revert !important; font-size: revert !important; font-size-adjust: revert !important; font-style: revert !important; font-synthesis-small-caps: revert !important; font-synthesis-style: revert !important; font-synthesis-weight: revert !important; font-variant-alternates: revert !important; font-variant-caps: revert !important; font-variant-east-asian: revert !important; font-variant-emoji: revert !important; font-variant-ligatures: revert !important; font-variant-numeric: revert !important; font-variant-position: revert !important; font-variation-settings: revert !important; font-weight: revert !important; font-width: revert !important; text-orientation: revert !important; text-rendering: revert !important; zoom: revert !important; -webkit-font-smoothing: revert !important; -webkit-locale: revert !important; -webkit-text-size-adjust: revert !important; -webkit-text-zoom: revert !important; letter-spacing: revert !important; text-autospace: revert !important; text-spacing-trim: revert !important; word-spacing: revert !important; background-image: revert !important; mask: revert !important; accent-color: revert !important; place-content: revert !important; place-items: revert !important; place-self: revert !important; alignment-baseline: revert !important; anchor-name: revert !important; anchor-scope: revert !important; animation-composition: revert !important; animation: revert !important; appearance: revert !important; aspect-ratio: revert !important; backdrop-filter: revert !important; backface-visibility: revert !important; background-attachment: revert !important; background-blend-mode: revert !important; background-clip: revert !important; background-origin: revert !important; background-position: revert !important; background-repeat: revert !important; background-size: revert !important; baseline-shift: revert !important; line-clamp: revert !important; block-step: revert !important; border-collapse: revert !important; border: revert !important; box-shadow: revert !important; box-sizing: revert !important; break-after: revert !important; break-before: revert !important; break-inside: revert !important; buffered-rendering: revert !important; caption-side: revert !important; caret-color: revert !important; clear: revert !important; clip: revert !important; clip-path: revert !important; clip-rule: revert !important; color: revert !important; color-interpolation: revert !important; color-interpolation-filters: revert !important; column-count: revert !important; column-fill: revert !important; gap: revert !important; column-rule-color: revert !important; column-rule-style: revert !important; column-rule-width: revert !important; column-span: revert !important; column-width: revert !important; contain: revert !important; container-name: revert !important; container-type: revert !important; content: revert !important; content-visibility: revert !important; counter-increment: revert !important; counter-reset: revert !important; counter-set: revert !important; cursor: revert !important; cx: revert !important; cy: revert !important; d: revert !important; dominant-baseline: revert !important; dynamic-range-limit: revert !important; empty-cells: revert !important; field-sizing: revert !important; fill: revert !important; fill-opacity: revert !important; fill-rule: revert !important; filter: revert !important; flex: revert !important; flex-flow: revert !important; float: revert !important; flood-color: revert !important; flood-opacity: revert !important; flow-tolerance: revert !important; glyph-orientation-horizontal: revert !important; glyph-orientation-vertical: revert !important; grid: revert !important; grid-column-end: revert !important; grid-column-start: revert !important; grid-row-end: revert !important; grid-row-start: revert !important; hanging-punctuation: revert !important; hyphenate-character: revert !important; hyphens: revert !important; image-orientation: revert !important; image-rendering: revert !important; input-security: revert !important; isolation: revert !important; lighting-color: revert !important; line-break: revert !important; line-fit-edge: revert !important; line-height: revert !important; list-style: revert !important; margin-trim: revert !important; marker: revert !important; mask-composite: revert !important; mask-mode: revert !important; mask-size: revert !important; mask-type: revert !important; math-shift: revert !important; math-style: revert !important; mix-blend-mode: revert !important; object-fit: revert !important; object-position: revert !important; offset-anchor: revert !important; offset-distance: revert !important; offset-path: revert !important; offset-position: revert !important; offset-rotate: revert !important; order: revert !important; orphans: revert !important; outline: revert !important; outline-offset: revert !important; overflow-anchor: revert !important; overflow-wrap: revert !important; page: revert !important; paint-order: revert !important; perspective: revert !important; perspective-origin: revert !important; pointer-events: revert !important; position: revert !important; position-anchor: revert !important; position-area: revert !important; position-try: revert !important; position-visibility: revert !important; print-color-adjust: revert !important; quotes: revert !important; r: revert !important; resize: revert !important; rotate: revert !important; ruby-align: revert !important; ruby-overhang: revert !important; rx: revert !important; ry: revert !important; scale: revert !important; scroll-behavior: revert !important; scroll-snap-align: revert !important; scroll-snap-stop: revert !important; scroll-snap-type: revert !important; scroll-timeline: revert !important; scrollbar-color: revert !important; scrollbar-gutter: revert !important; scrollbar-width: revert !important; shape-image-threshold: revert !important; shape-margin: revert !important; shape-outside: revert !important; shape-rendering: revert !important; speak-as: revert !important; stop-color: revert !important; stop-opacity: revert !important; stroke: revert !important; stroke-color: revert !important; stroke-dasharray: revert !important; stroke-dashoffset: revert !important; stroke-linecap: revert !important; stroke-linejoin: revert !important; stroke-miterlimit: revert !important; stroke-opacity: revert !important; stroke-width: revert !important; tab-size: revert !important; table-layout: revert !important; text-align: revert !important; text-align-last: revert !important; text-anchor: revert !important; text-box: revert !important; text-combine-upright: revert !important; text-decoration: revert !important; text-decoration-skip-ink: revert !important; text-emphasis-color: revert !important; text-emphasis-position: revert !important; text-emphasis-style: revert !important; text-group-align: revert !important; text-indent: revert !important; text-justify: revert !important; text-overflow: revert !important; text-shadow: revert !important; text-transform: revert !important; text-underline-offset: revert !important; text-underline-position: revert !important; text-wrap: revert !important; timeline-scope: revert !important; touch-action: revert !important; transform: revert !important; transform-box: revert !important; transform-origin: revert !important; transform-style: revert !important; transition: revert !important; translate: revert !important; vector-effect: revert !important; vertical-align: revert !important; view-timeline: revert !important; view-transition-class: revert !important; view-transition-name: revert !important; white-space: revert !important; widows: revert !important; will-change: revert !important; word-break: revert !important; x: revert !important; y: revert !important; z-index: revert !important; -apple-color-filter: revert !important; -apple-pay-button-style: revert !important; -apple-pay-button-type: revert !important; -apple-visual-effect: revert !important; -internal-text-autosizing-status: revert !important; -webkit-backdrop-filter: revert !important; -webkit-background-clip: revert !important; -webkit-background-origin: revert !important; border-spacing: revert !important; -webkit-box-align: revert !important; -webkit-box-decoration-break: revert !important; -webkit-box-direction: revert !important; -webkit-box-flex: revert !important; -webkit-box-flex-group: revert !important; -webkit-box-lines: revert !important; -webkit-box-ordinal-group: revert !important; -webkit-box-orient: revert !important; -webkit-box-pack: revert !important; -webkit-box-reflect: revert !important; -webkit-box-shadow: revert !important; -webkit-column-axis: revert !important; -webkit-column-progression: revert !important; -webkit-cursor-visibility: revert !important; -webkit-font-size-delta: revert !important; -webkit-hyphenate-limit-after: revert !important; -webkit-hyphenate-limit-before: revert !important; -webkit-hyphenate-limit-lines: revert !important; -webkit-initial-letter: revert !important; -webkit-line-align: revert !important; -webkit-line-box-contain: revert !important; -webkit-line-clamp: revert !important; -webkit-line-grid: revert !important; -webkit-line-snap: revert !important; -webkit-marquee-direction: revert !important; -webkit-marquee-increment: revert !important; -webkit-marquee-repetition: revert !important; -webkit-marquee-speed: revert !important; -webkit-marquee-style: revert !important; -webkit-mask: revert !important; -webkit-mask-composite: revert !important; -webkit-mask-source-type: revert !important; -webkit-nbsp-mode: revert !important; -webkit-overflow-scrolling: revert !important; -webkit-rtl-ordering: revert !important; -webkit-ruby-position: revert !important; -webkit-tap-highlight-color: revert !important; -webkit-text-combine: revert !important; -webkit-text-decorations-in-effect: revert !important; -webkit-text-fill-color: revert !important; -webkit-text-security: revert !important; -webkit-text-stroke-color: revert !important; -webkit-text-stroke-width: revert !important; -webkit-touch-callout: revert !important; -webkit-user-drag: revert !important; -webkit-user-modify: revert !important; -webkit-user-select: revert !important; border-radius: revert !important; inset: revert !important; contain-intrinsic-size: revert !important; corner-shape: revert !important; height: revert !important; margin: revert !important; min-height: revert !important; min-width: revert !important; overflow: revert !important; overscroll-behavior: revert !important; padding: revert !important; scroll-margin: revert !important; scroll-padding: revert !important; width: revert !important; block-size: revert !important; border-block: revert !important; border-end-end-radius: revert !important; border-end-start-radius: revert !important; border-inline: revert !important; border-start-end-radius: revert !important; border-start-start-radius: revert !important; contain-intrinsic-block-size: revert !important; contain-intrinsic-inline-size: revert !important; corner-end-end-shape: revert !important; corner-end-start-shape: revert !important; corner-start-end-shape: revert !important; corner-start-start-shape: revert !important; inline-size: revert !important; inset-block: revert !important; inset-inline: revert !important; margin-block: revert !important; margin-inline: revert !important; max-block-size: revert !important; max-inline-size: revert !important; min-block-size: revert !important; min-inline-size: revert !important; overflow-block: revert !important; overflow-inline: revert !important; overscroll-behavior-block: revert !important; overscroll-behavior-inline: revert !important; padding-block: revert !important; padding-inline: revert !important; scroll-margin-block: revert !important; scroll-margin-inline: revert !important; scroll-padding-block: revert !important; scroll-padding-inline: revert !important; display: block !important; visibility: visible !important; opacity: 1 !important; background-color: rgb(208, 216, 220) !important; max-width: none !important; max-height: none !important; }
.pfptPrimaryButtonud867qm:hover, .pfptPrimaryButtonud867qm:focus { background-color: rgb(180, 193, 199) !important; }
.pfptPrimaryButtonud867qm:active { background-color: rgb(144, 164, 174) !important; }
html:root, html:root > body { color-scheme: revert !important; math-depth: revert !important; ruby-position: revert !important; writing-mode: revert !important; font-family: revert !important; font-feature-settings: revert !important; font-kerning: revert !important; font-optical-sizing: revert !important; font-palette: revert !important; font-size: revert !important; font-size-adjust: revert !important; font-style: revert !important; font-synthesis-small-caps: revert !important; font-synthesis-style: revert !important; font-synthesis-weight: revert !important; font-variant-alternates: revert !important; font-variant-caps: revert !important; font-variant-east-asian: revert !important; font-variant-emoji: revert !important; font-variant-ligatures: revert !important; font-variant-numeric: revert !important; font-variant-position: revert !important; font-variation-settings: revert !important; font-weight: revert !important; font-width: revert !important; text-orientation: revert !important; text-rendering: revert !important; zoom: revert !important; -webkit-font-smoothing: revert !important; -webkit-locale: revert !important; -webkit-text-size-adjust: revert !important; -webkit-text-zoom: revert !important; letter-spacing: revert !important; text-autospace: revert !important; text-spacing-trim: revert !important; word-spacing: revert !important; background: revert !important; mask: revert !important; accent-color: revert !important; place-content: revert !important; place-items: revert !important; place-self: revert !important; alignment-baseline: revert !important; anchor-name: revert !important; anchor-scope: revert !important; animation-composition: revert !important; animation: revert !important; appearance: revert !important; aspect-ratio: revert !important; backdrop-filter: revert !important; backface-visibility: revert !important; background-blend-mode: revert !important; baseline-shift: revert !important; line-clamp: revert !important; block-step: revert !important; border-collapse: revert !important; border: revert !important; box-shadow: revert !important; box-sizing: revert !important; break-after: revert !important; break-before: revert !important; break-inside: revert !important; buffered-rendering: revert !important; caption-side: revert !important; caret-color: revert !important; clear: revert !important; clip: revert !important; clip-path: revert !important; clip-rule: revert !important; color: revert !important; color-interpolation: revert !important; color-interpolation-filters: revert !important; column-count: revert !important; column-fill: revert !important; gap: revert !important; column-rule-color: revert !important; column-rule-style: revert !important; column-rule-width: revert !important; column-span: revert !important; column-width: revert !important; contain: revert !important; container-name: revert !important; container-type: revert !important; content: revert !important; content-visibility: revert !important; counter-increment: revert !important; counter-reset: revert !important; counter-set: revert !important; cursor: revert !important; cx: revert !important; cy: revert !important; d: revert !important; dominant-baseline: revert !important; dynamic-range-limit: revert !important; empty-cells: revert !important; field-sizing: revert !important; fill: revert !important; fill-opacity: revert !important; fill-rule: revert !important; filter: revert !important; flex: revert !important; flex-flow: revert !important; float: revert !important; flood-color: revert !important; flood-opacity: revert !important; flow-tolerance: revert !important; glyph-orientation-horizontal: revert !important; glyph-orientation-vertical: revert !important; grid: revert !important; grid-column-end: revert !important; grid-column-start: revert !important; grid-row-end: revert !important; grid-row-start: revert !important; hanging-punctuation: revert !important; hyphenate-character: revert !important; hyphens: revert !important; image-orientation: revert !important; image-rendering: revert !important; input-security: revert !important; isolation: revert !important; lighting-color: revert !important; line-break: revert !important; line-fit-edge: revert !important; line-height: revert !important; list-style: revert !important; margin-trim: revert !important; marker: revert !important; mask-composite: revert !important; mask-mode: revert !important; mask-size: revert !important; mask-type: revert !important; math-shift: revert !important; math-style: revert !important; mix-blend-mode: revert !important; object-fit: revert !important; object-position: revert !important; offset-anchor: revert !important; offset-distance: revert !important; offset-path: revert !important; offset-position: revert !important; offset-rotate: revert !important; order: revert !important; orphans: revert !important; outline: revert !important; outline-offset: revert !important; overflow-anchor: revert !important; overflow-wrap: revert !important; page: revert !important; paint-order: revert !important; perspective: revert !important; perspective-origin: revert !important; pointer-events: revert !important; position: revert !important; position-anchor: revert !important; position-area: revert !important; position-try: revert !important; position-visibility: revert !important; print-color-adjust: revert !important; quotes: revert !important; r: revert !important; resize: revert !important; rotate: revert !important; ruby-align: revert !important; ruby-overhang: revert !important; rx: revert !important; ry: revert !important; scale: revert !important; scroll-behavior: revert !important; scroll-snap-align: revert !important; scroll-snap-stop: revert !important; scroll-snap-type: revert !important; scroll-timeline: revert !important; scrollbar-color: revert !important; scrollbar-gutter: revert !important; scrollbar-width: revert !important; shape-image-threshold: revert !important; shape-margin: revert !important; shape-outside: revert !important; shape-rendering: revert !important; speak-as: revert !important; stop-color: revert !important; stop-opacity: revert !important; stroke: revert !important; stroke-color: revert !important; stroke-dasharray: revert !important; stroke-dashoffset: revert !important; stroke-linecap: revert !important; stroke-linejoin: revert !important; stroke-miterlimit: revert !important; stroke-opacity: revert !important; stroke-width: revert !important; tab-size: revert !important; table-layout: revert !important; text-align: revert !important; text-align-last: revert !important; text-anchor: revert !important; text-box: revert !important; text-combine-upright: revert !important; text-decoration: revert !important; text-decoration-skip-ink: revert !important; text-emphasis-color: revert !important; text-emphasis-position: revert !important; text-emphasis-style: revert !important; text-group-align: revert !important; text-indent: revert !important; text-justify: revert !important; text-overflow: revert !important; text-shadow: revert !important; text-transform: revert !important; text-underline-offset: revert !important; text-underline-position: revert !important; text-wrap: revert !important; timeline-scope: revert !important; touch-action: revert !important; transform: revert !important; transform-box: revert !important; transform-origin: revert !important; transform-style: revert !important; transition: revert !important; translate: revert !important; vector-effect: revert !important; vertical-align: revert !important; view-timeline: revert !important; view-transition-class: revert !important; view-transition-name: revert !important; white-space: revert !important; widows: revert !important; will-change: revert !important; word-break: revert !important; x: revert !important; y: revert !important; z-index: revert !important; -apple-color-filter: revert !important; -apple-pay-button-style: revert !important; -apple-pay-button-type: revert !important; -apple-visual-effect: revert !important; -internal-text-autosizing-status: revert !important; -webkit-backdrop-filter: revert !important; -webkit-background-clip: revert !important; -webkit-background-origin: revert !important; border-spacing: revert !important; -webkit-box-align: revert !important; -webkit-box-decoration-break: revert !important; -webkit-box-direction: revert !important; -webkit-box-flex: revert !important; -webkit-box-flex-group: revert !important; -webkit-box-lines: revert !important; -webkit-box-ordinal-group: revert !important; -webkit-box-orient: revert !important; -webkit-box-pack: revert !important; -webkit-box-reflect: revert !important; -webkit-box-shadow: revert !important; -webkit-column-axis: revert !important; -webkit-column-progression: revert !important; -webkit-cursor-visibility: revert !important; -webkit-font-size-delta: revert !important; -webkit-hyphenate-limit-after: revert !important; -webkit-hyphenate-limit-before: revert !important; -webkit-hyphenate-limit-lines: revert !important; -webkit-initial-letter: revert !important; -webkit-line-align: revert !important; -webkit-line-box-contain: revert !important; -webkit-line-clamp: revert !important; -webkit-line-grid: revert !important; -webkit-line-snap: revert !important; -webkit-marquee-direction: revert !important; -webkit-marquee-increment: revert !important; -webkit-marquee-repetition: revert !important; -webkit-marquee-speed: revert !important; -webkit-marquee-style: revert !important; -webkit-mask: revert !important; -webkit-mask-composite: revert !important; -webkit-mask-source-type: revert !important; -webkit-nbsp-mode: revert !important; -webkit-overflow-scrolling: revert !important; -webkit-rtl-ordering: revert !important; -webkit-ruby-position: revert !important; -webkit-tap-highlight-color: revert !important; -webkit-text-combine: revert !important; -webkit-text-decorations-in-effect: revert !important; -webkit-text-fill-color: revert !important; -webkit-text-security: revert !important; -webkit-text-stroke-color: revert !important; -webkit-text-stroke-width: revert !important; -webkit-touch-callout: revert !important; -webkit-user-drag: revert !important; -webkit-user-modify: revert !important; -webkit-user-select: revert !important; border-radius: revert !important; inset: revert !important; contain-intrinsic-size: revert !important; corner-shape: revert !important; height: revert !important; margin: revert !important; max-height: revert !important; max-width: revert !important; min-height: revert !important; min-width: revert !important; overflow: revert !important; overscroll-behavior: revert !important; padding: revert !important; scroll-margin: revert !important; scroll-padding: revert !important; width: revert !important; block-size: revert !important; border-block: revert !important; border-end-end-radius: revert !important; border-end-start-radius: revert !important; border-inline: revert !important; border-start-end-radius: revert !important; border-start-start-radius: revert !important; contain-intrinsic-block-size: revert !important; contain-intrinsic-inline-size: revert !important; corner-end-end-shape: revert !important; corner-end-start-shape: revert !important; corner-start-end-shape: revert !important; corner-start-start-shape: revert !important; inline-size: revert !important; inset-block: revert !important; inset-inline: revert !important; margin-block: revert !important; margin-inline: revert !important; max-block-size: revert !important; max-inline-size: revert !important; min-block-size: revert !important; min-inline-size: revert !important; overflow-block: revert !important; overflow-inline: revert !important; overscroll-behavior-block: revert !important; overscroll-behavior-inline: revert !important; padding-block: revert !important; padding-inline: revert !important; scroll-margin-block: revert !important; scroll-margin-inline: revert !important; scroll-padding-block: revert !important; scroll-padding-inline: revert !important; display: block !important; visibility: visible !important; opacity: 1 !important; }</style><!-- BaNnErBlUrFlE-HeAdEr-end -->
<div style="font-family: inherit; font-size: inherit; color: rgb(0, 0, 0); background-color: transparent;">
</div>
<div style="font-family: inherit; font-size: inherit; color: rgb(0, 0, 0); background-color: transparent;">
Hi Amir,</div>
<div style="font-family: inherit; font-size: inherit; color: rgb(0, 0, 0); background-color: transparent;">
We get ours from Dischem (2%, 4%, 16%, and 20%). They call it HSiQ.</div>
<div style="font-family: inherit; font-size: inherit; color: rgb(0, 0, 0); background-color: transparent;">
<br>
</div>
<div style="font-family: inherit; font-size: inherit; color: rgb(0, 0, 0); background-color: transparent;">
The contact is Andy Thompson, andy@dischem.com. They are in Pittsburgh and mix it on order, but the resin comes from Canada so there is sometimes a tariff fee. He’ll make small quantities so you don’t have to order a liter each time.</div>
<div style="font-family: inherit; font-size: inherit; color: rgb(0, 0, 0); background-color: transparent;">
<br>
</div>
<div style="font-family: inherit; font-size: inherit; color: rgb(0, 0, 0); background-color: transparent;">
Aimee</div>
<hr style="display:inline-block;width:98%" tabindex="-1">
<div id="divRplyFwdMsg" dir="ltr"><font face="Calibri, sans-serif" style="font-size:11pt" color="#000000"><b>From:</b> labnetwork <labnetwork-bounces@mtl.mit.edu> on behalf of Amir Safavi-Naeini <safavi@stanford.edu><br>
<b>Sent:</b> Tuesday, August 11, 2026 5:01 PM<br>
<b>To:</b> labnetwork@mtl.mit.edu <labnetwork@mtl.mit.edu><br>
<b>Cc:</b> Taewon Park <twpark@stanford.edu><br>
<b>Subject:</b> [labnetwork] Current source for HSQ (FOx-16 / XR-1541)?</font>
<div> </div>
</div>
<style>#x_pfptBannerc5ph7zk { display: block !important; visibility: visible !important; opacity: 1 !important; background-color: rgb(207, 211, 215) !important; max-width: none !important; max-height: none !important; }
html:root, html:root > div { display: block !important; visibility: visible !important; opacity: 1 !important; }</style>
<div>
<div style="display:none!important; display:none; visibility:hidden; font-size:1px; color:#ffffff; line-height:1px; max-height:0px; opacity:0; overflow:hidden">
Hi everyone, We use HSQ as our high-resolution negative e-beam resist at Stanford, mostly for nanophotonic and quantum devices in lithium niobate and silicon. We've been trying to restock and have not been able to find a current source. </div>
<div style="display:none!important; display:none; visibility:hidden; font-size:1px; color:#ffffff; line-height:1px; max-height:0px; opacity:0; overflow:hidden">
</div>
<div dir="ltr">
<div>
<div dir="auto">Hi everyone,<br>
<br>
We use HSQ as our high-resolution negative e-beam resist at Stanford, mostly for nanophotonic and quantum devices in lithium niobate and silicon. We've been trying to restock and have not been able to find a current source.<br>
<br>
Two questions:<br>
<br>
1. Where are people buying HSQ these days? FOx-16, FOx-25, XR-1541, or any equivalent formulation. A vendor name and a contact would be enormously helpful. We only need a liter or two every year or two, so we are not a large-volume customer and that may be
part of the problem.<br>
<br>
2. If the supply situation is genuinely dead, what are people using instead for high-resolution negative-tone work, and what did you give up in switching?<br>
<br>
For what it's worth, we store ours in LN2, so shelf life isn't our limiting factor we believe... <br>
<br>
Happy to summarize replies back to the list if there's interest.<br>
<br>
Thanks,<br>
Amir<br>
</div>
</div>
<div><br>
</div>
<span class="x_gmail_signature_prefix">-- </span><br>
<div dir="ltr" class="x_gmail_signature" data-smartmail="gmail_signature">
<div dir="ltr">
<div>
<div dir="ltr">Amir H. Safavi-Naeini<br>
Associate Professor<br>
Department of Applied Physics<br>
Ginzton Laboratory, Stanford University<br>
<br>
mail address:<br>
</div>
<div dir="ltr">
<div dir="ltr">Edward L. Ginzton Laboratory</div>
<div dir="ltr">348 Via Pueblo Mall, Box 336</div>
<div dir="ltr">Stanford University</div>
<div dir="ltr">Stanford, CA 94305-4088</div>
<div><br>
</div>
</div>
<div dir="ltr">office phone: +1 650 498 7496 [Room 309, Spilker]<br>
mobile phone: +1 626 379 3702<br>
zoom: <a href="https://urldefense.com/v3/__https://stanford.zoom.us/j/4970959839__;!!KGKeukY!3-rGPu-irtPthXqithYAG3cfY_w_fYvxpzyUe7FkHGQbiKYnmEyvpPsu9-wCvHY9CAbJEgfTULe2joQIq7sxQA$" target="_blank">
https://stanford.zoom.us/j/4970959839</a>
<div><a href="https://urldefense.com/v3/__http://www.stanford.edu/*safavi/__;fg!!KGKeukY!3-rGPu-irtPthXqithYAG3cfY_w_fYvxpzyUe7FkHGQbiKYnmEyvpPsu9-wCvHY9CAbJEgfTULe2joToTYNPtQ$" target="_blank">http://www.stanford.edu/~safavi/</a><br>
-------------------------------------------------</div>
</div>
</div>
</div>
</div>
</div>
</div>
<span>_______________________________________________</span><br>
<span>labnetwork mailing list</span><br>
<span>labnetwork@mtl.mit.edu</span><br>
<span>https://urldefense.com/v3/__https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork__;!!K-Hz7m0Vt54!ixRxrF4HDYgXAPx0QsrY_Sm5AiLW4JevE91m5MMQ2ie6unDxlq4as97GHftB3miTy0roaNyg4ckJnBQqyw$
</span><br>
</div>
</blockquote>
</div>
</body>
</html>