[labnetwork] Dektak 3030ST - stylus down timeout error
Teynor, William A.
wteynor at draper.com
Mon Sep 18 12:10:20 EDT 2017
Dear Kevin,
>From an Dektak 3030 manual found online...
4. "Stylus Down Timeout." This signifies that the stylus mechanism has not stabilized on
sample surface, within specified time limit initiated by a "scan" or "stylus down"
command. Reduce travel distance between stylus and sample surface and try again.
Hope this helps.
Regards,
Bill
William A. Teynor
Senior Member of the Technical Staff
Draper
555 Technology Square
Cambridge, MA
02139-3573
Work 617-258-4289
Cell 617-529-8942
www.draper.com
-----Original Message-----
From: labnetwork-bounces at mtl.mit.edu [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Fouad Karouta
Sent: Sunday, September 17, 2017 7:19 PM
To: Kevin McPeak <kmcpeak at lsu.edu>; labnetwork at mtl.mit.edu
Subject: Re: [labnetwork] Dektak 3030ST - stylus down timeout error
Dear Kevin,
We had 2 years ago an issue with our Dektak XT but I don't recall the error message. The problem was the stylus went all the way down touching the sample to measure and going immediately all the way up again. No scans were possible. We had to call a Dektak engineer and they had to replace an electronic control card.
Regards,
Fouad Karouta
*************************************
Manager ANFF ACT Node
Australian National Fabrication Facility Research School of Physics and Engineering L. Huxley Building (#56), Mills Road, Room 4.02 Australian National University ACT 0200, Canberra, Australia
Tel: + 61 2 6125 7174
Mob: + 61 451 046 412
Email: fouad.karouta at anu.edu.au<mailto:fouad.karouta at anu.edu.au>
http://anff-act.anu.edu.au/
-----Original Message-----
From: labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu> [mailto:labnetwork-bounces at mtl.mit.edu] On Behalf Of Kevin McPeak
Sent: Sunday, 17 September 2017 1:30 PM
To: labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
Subject: [labnetwork] Dektak 3030ST - stylus down timeout error
Dear Colleagues,
The Dektak 3030ST contact profilometer here at LSU is giving a "Stylus Down Timeout" error. As a result, the system will not perform any scans.
Have any of you observed this error before and if so how did you resolve it.
Regards,
Kevin
--
Kevin M. McPeak
Assistant Professor
Louisiana State University
Dept. of Chemical Engineering
110 Chemical Engineering Bldg Room 324
S. Stadium Drive
Baton Rouge, LA 70803
email: kmcpeak at lsu.edu<mailto:kmcpeak at lsu.edu>
phone: 225-578-0058
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
________________________________
Notice: This email and any attachments may contain proprietary (Draper non-public) and/or export-controlled information of Draper. If you are not the intended recipient of this email, please immediately notify the sender by replying to this email and immediately destroy all copies of this email.
________________________________
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20170918/d33d44d9/attachment.html>
More information about the labnetwork
mailing list