Good morning Ahad,

we had the same problem here in Germany to find a reliable source of 
XeF2. While we received our first supply from BOC in Britain in 2015, we 
were struggling to get a refill in 2017. At that time Linde had issued a 
press release that they had signed an agreement to import XeF2 from the 
manufacturer Pelchem and supply end users, but that seems to apply only 
for the US. Linde Germany could not help us. We tried a couple of other 
chemical companies dealing with XeF2 we found in the web, but nobody was 
really able to deliver the purity we wanted in the container fitted to 
the machine. In the end we were served well by the XeF2 manufacturer in 
South Africa. As it looks like you can purchase there directly. The only 
problem we had is getting the container there and back through customs 
without paying duties on the container. At Pelchem we dealt with Nerona 
Naidoo, email Nerona.Naidoo at pelchem.necsa.co.za. Pelchem details are 
attached as jpg. Turnaround time was about 4 to 6 weeks while the custom 
procedures took most of the time.

Good luck
Michael Wandt


Am 21.10.2018 um 16:10 schrieb Ahad Syed:
>
> ​Dear Colleagues,
>
>
> We are looking for reliable suppliers for XeF2 for our Xactix X3C. Our 
> supplier for the past 10 years has decided to remove XeF2 from his 
> catalog. We are looking at lead times less than 4-5 months. Your 
> suggestions will be highly appreciated.
>
>
> Thank you,
>
> Ahad
>
> ​
>
> --
> Nanofabrication Core Lab
> 4700 King Abdullah University of Science and Technology
> 0247 Building 3, Thuwal 23955-6900, Kingdom of Saudi Arabia
> Tel:+966 12 808 2348
> Visit The Core Labs <https://corelabs.kaust.edu.sa/visitor-information>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork

-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20181022/9e21ac9d/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: Pelchem_Details.jpg
Type: image/jpeg
Size: 16893 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20181022/9e21ac9d/attachment.jpg>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: michael_wandt.vcf
Type: text/x-vcard
Size: 391 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20181022/9e21ac9d/attachment.vcf>


More information about the labnetwork mailing list