Hi Jorg,
We have gotten laser hole drilling in Pyrex from AdValue Tech. They also
machine many other substrates.
Their website is:
https://www.advaluetech.com/laser/
Regards,
Caleb
On Thu, Aug 20, 2020 at 8:15 AM Jorg Scholvin <scholvin at mit.edu> wrote:
> Hi Labnetwork:
>
>
>
> We have recently gotten a couple of requests from users at MIT.nano for
> laser micromachining -- ablating holes through pyrex, Si, or AlN substrates.
>
>
>
> We currently don’t have suitable capabilities. If you offer
> remote/staff-run services, or if you know of a company that offers
> capabilities, we’d love to know and refer our researchers that way.
>
>
>
> Thanks!
>
>
>
> -Jorg
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20200820/077abd92/attachment.html>
More information about the labnetwork
mailing list