[labnetwork] XeF2 supplier?
mtkhbeis at gmail.com
mtkhbeis at gmail.com
Tue Feb 4 16:46:32 EST 2020
John
Is Pelchem non-responsive? I had difficulty last time because the POC listed was on long term leave. I managed to finally get a response by finding other POCs via LinkedIn. We ended up sourcing via Air Products since they stocked material.
Good luck,
Dr. Michael Khbeis
(C) 443.254.5192
> On Feb 4, 2020, at 9:23 AM, John Nash <jcn8004 at rit.edu> wrote:
>
>
> Does anyone know of a reliable supplier of XeF2? We have a Xactics XeF2 system that will be running out soon. I have reached out to Pelchem, Electronic fluorocarbons and Linde over the last 6 months and none are able to help. Thanks in advance for all recommendations.
>
> Regards,
>
> John C Nash
> SMFL - Technician
> Rochester Institute of Technology
> Semiconductor & Microsystems Fabrication Laboratory
> 82 Lomb Memorial Dr.
> Bldg. 17-2627
> Rochester, NY 14623
>
> 585 478-3835 cell
> john.nash at rit.edu
> www.smfl.rit.edu
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20200204/a195523c/attachment.html>
More information about the labnetwork
mailing list