[labnetwork] O2 8%/CF4 gas cylinder
James Mitchell
jtmitch5 at ncsu.edu
Tue Feb 14 01:05:41 EST 2023
Have you tried Airgas?
Jim
On Mon, Feb 13, 2023, 5:37 PM John Tamelier <jtamelier at eng.ucsd.edu> wrote:
> Hello all,
>
> We have been having difficulty getting a cylinder of O2 8%/CF4. We
> placed an order in early November 2022 with Linde and have yet to
> receive a ship date for the material. We have three orders out, but need
> the material urgently. The shortest lead time we have found is 9 weeks.
>
> Does anyone have any contacts for purchasing this gas or other options
> for obtaining a cylinder of this gas? Is anyone else experiencing this
> type of lead time for gas cylinders?
>
> Thank you,
>
> John
>
> -----------------------------------
> John Tamelier, Ph.D.
> Interim Director - Nano3
>
> University of California, San Diego
> Atkinson Hall, 5th Floor Front Desk, M/C 0436
> 9500 Gilman Drive
> La Jolla, California 92093-0436
> Phone: (858) 246-2735
> Fax: (858) 534-9092
> E-mail: jtamelier at ucsd.edu
> http://nano3.calit2.net
> ----------------------------------
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20230214/32a79a99/attachment.html>
More information about the labnetwork
mailing list