[labnetwork] Powder blasting for micromachining
Philipp Altpeter
philipp.altpeter at lmu.de
Wed Oct 25 13:45:45 EDT 2023
Dear labnetwork,
We're currently looking for a way to pattern glass with a high etch rate, and micro powder blasting looks like an excellent candidate.
Can you recommend a manufacturer of powder blasting machines suited for micro machining of glass (BSG)?
We work on rather small wafer sizes, down to single dices with lateral dimensions of a few mm.
Thank you so much in advance!
Philipp
--
Philipp Altpeter
Fakultät für Physik der LMU
LS Prof. Efetov
Geschwister-Scholl-Platz 1
D-80539 München
T. +49 (0)89 2180-3733