[labnetwork] Looking for other labs with mid 2000's era deposition MVD100 tool

Sam Tsitrin samtsitrin at berkeley.edu
Fri Oct 11 19:06:24 EDT 2024


Hello labnetwork-
We are having a hard time repairing our molecular vapor deposition tool
MVD100 from Applied Micro Systems. This is used for FOTS coating
primarily.  The issue seems to be software related, specifically with the
GV52 HMI unit used to control the tool.
If you have a similar vintage MVD100 and are willing to help, please reach
out.
Much appreciated,


-- 
Sam Tsitrin

R&D Engineer
UC Berkeley Marvell Nanolab