[labnetwork] PDMS processing - separate lab?
Kyle Keenan
kckeenan at seas.upenn.edu
Wed Sep 4 14:59:32 EDT 2024
Hi Dan,
Short answer for us: we have a newly dedicated space for this in a remote
part of the cleanroom. There are special protocols for using this space
(special disposable gloves, blue sticky mats, signage) to minimize the
impact on adjacent spaces, as well as the rest of the cleanroom.
Best,
Kyle
On Wed, Sep 4, 2024 at 2:52 PM Dan P. Woodie <daniel.woodie at princeton.edu>
wrote:
> Lab Network,
>
>
>
> I am curious how many fabs allow PDMS mixing in their main cleanrooms and
> how many require that work done in separate isolated spaces or noncleanroom
> labs. My experience has been that they can be in the same space if careful
> glove protocols are used to avoid spreading the unpolymerized precursors
> around the facility, but I am interested in other’s experiences. Thanks for
> the shared knowledge.
>
>
>
> Dan
>
>
>
> Daniel Woodie
>
> Director, Micro/Nano Fabrication Center, Princeton Materials Institute
>
> Princeton University
>
> 155 Andlinger Center
>
> 86 Olden St
>
> Princeton, NJ 08540
>
>
>
> (609)258-5922 (office)
>
> (607)227-2993 (cell)
>
> daniel.woodie at princeton.edu
>
> mnfc.princeton.edu
> <https://urldefense.com/v3/__https://mnfc.princeton.edu/__;!!IBzWLUs!RIQyUlg3VITVgCvRMG_LaZS5r3x23wcF4Zguzt_ANezoxyGVohfMt2jaiZkdrydiuaLvloUine4mMdLKOlbmAZ5xxfaP1TVxpg$>
>
> www.linkedin.com/in/danielpwoodie
> <https://urldefense.com/v3/__http://www.linkedin.com/in/danielpwoodie/__;!!IBzWLUs!RIQyUlg3VITVgCvRMG_LaZS5r3x23wcF4Zguzt_ANezoxyGVohfMt2jaiZkdrydiuaLvloUine4mMdLKOlbmAZ5xxfZnkzO8lg$>
>
>
>
>
>
>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
>
> https://urldefense.com/v3/__https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork__;!!IBzWLUs!RIQyUlg3VITVgCvRMG_LaZS5r3x23wcF4Zguzt_ANezoxyGVohfMt2jaiZkdrydiuaLvloUine4mMdLKOlbmAZ5xxfagd8Gkvg$
>
--
Kyle Keenan
Senior Manager - Laboratory Operations
Quattrone Nanofabrication Facility
University of Pennsylvania
P: 215-898-7560
F: 215-573-4925
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20240904/f8dc6a76/attachment.html>
More information about the labnetwork
mailing list