Hi Jeff,

We've had communication issues twice before with our Dektak 150.  Both times it was a failure of this $80-90 converter:
https://www.coolgear.com/product/single-port-usb-to-rs422-485-adapter
Bruker will offer to sell you the exact same item for $400-$500.

If it were me, I'd try replacing that before going down the service route.

Best,
Travis Massey
Lawrence Livermore National Laboratory

From: labnetwork <labnetwork-bounces at mtl.mit.edu> On Behalf Of Jeff Salzmann
Sent: Tuesday, February 18, 2025 7:59 AM
To: Fab Network <labnetwork at mtl.mit.edu>
Subject: [labnetwork] Looking for vendor service- Veeco/Dektak 150

My recently refurbished stylus profilometer is having communication issues. Might anyone have a recommendation for a company that can service these systems?

Thanks!!!!

Jeff

Jeff Salzmann
Assistant Professor of Research
Cleanroom Manager, Shared Instrumentation Laboratories
School of Engineering and Applied Sciences
University at Buffalo
114A Davis Hall
Buffalo, NY 14260
Tel: 716.645.2584

-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20250218/bf9f2202/attachment.html>


More information about the labnetwork mailing list