Hi Christian,

Thank you for your insights... we will do some experiments with various PEEK fills and lattice structures and do the inspections you have suggested.  Also perhaps some testing in a vacuum chamber with qcm or mass spec.  Will let you know how it turns out in a few months.

Regards,

John H
Sent from my iPhone

> On Jan 4, 2025, at 10:30 AM, Christian Spoerl <christian.spoerl at idonus.com> wrote:
> 
> Dear John,
> 
> I have not done but I do see the following:
> * Critical point for vacuum chamber use are voids created when one polymer fiber does not fully connect (in volume) to the neighbor fiber during the printing process.
> 
> * To be able to judge this use your target printing process parameters and print a similar complexity real part. Then cut a section and make a visual inspection of the fiber - void structure by use of a simple binocular microscope.
> If you do not see any voids I would judge the part as vacuum chamber compatible. Else wise not.
> 
> * Furthermore you have to deal with your hollow structure.
> Either you print with 100% volume or you have to drill after printing some ventilation holes.
> 
> All comes down to how well you can handle your process and prevent voids and not ventilated areas. In principle it should be feasible.
> 
> Good luck & best regards
> Christian
> 
> PS: My guess is 50% chance and I am very curious about the result !
> 
> Christian Spoerl
> Managing Director
> 
> idonus sarl
> Rouges-Terres 61
> 2068 Hauterive / Neuchatel
> Switzerland
> tel: +41 32 724 44 40
> email: christian.spoerl at idonus.com
> www.idonus.com
> 
>> On 23.12.2024 16:14, John Hagopian wrote:
>> Does anyone have experience, (good or bad) with this unit?
>> 
>> Any information on vacuum compatibility of PEEK printed parts?
>> 
>> Thanks,
>> 
>> John Hagopian
>> Advanced Nanophotonics. LLC
>> 
>> _______________________________________________
>> labnetwork mailing list
>> labnetwork at mtl.mit.edu
>> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
> 
> 
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork




More information about the labnetwork mailing list