[labnetwork] Au electroplating, Vasu, CeNSE, IISc

Wolfgang Harneit wharneit at uos.de
Mon Jun 16 06:14:55 EDT 2025


Hello,

M-O-T seems to be a specialist in electroplating, so I bet you could ask 
them anything about processes and safety.

info at m-o-t.info

Best regards,

Wolfgang

On 14.06.25 07:04, Srinivasan Raghavan wrote:
>
> Hi labnetwork,
>
>   * This question pertains to Au electrodeposition. A cyanide based
>     plating solution is more stable than a sulfite based one but the
>     latter is preferred due to safety concerns. We use a sulfite bath
>     but have been experienced instability with solutions from at least
>     two vendors. The Au precipitates out. We are thinking of switching
>     to a cyanide bath.
>   * Does anyone use a MOT-GmbH tool of the kind pictured  below for Au
>     plating from a cyanide bath? While this tool has exhaust it is not
>     placed inside of a fume hood. Hence, we want to double check, to
>     see if anyone has used this configuration for Au plating from
>     cyanide solutions, their experience and the safety precautions
>     that were being taken.
>
> Thanks in advance.
>
> Regards
>
> Vasu
>
> Srinivasan Raghavan (Vasu)
>
> sraghavan at iisc.ac.in
>
> Professor
>
> Centre for Nano Science and Engineering (CeNSE)
>
> IISc, Bengaluru, 560012, India
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork

-- 
Prof. Dr. Wolfgang Harneit
Universität Osnabrück, Fachbereich Mathematik/Informatik/Physik
Institut für Physik, Barbarastr. 7, 49076 Osnabrück, Germany
www.quantum-spintronics.de,www.molecular-spintronics.de
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20250616/6aa16b68/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 645103 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20250616/6aa16b68/attachment.png>


More information about the labnetwork mailing list