[labnetwork] [EXTERNAL] Re: Photomask Manufacturing Companies

Alex Dixon agdixon at mines.edu
Wed Mar 5 20:05:16 EST 2025


We have used Front Range Photomask ( https://www.frontrangephotomask.com/ ) The masks come out well and they have quick turnaround.
-Alex
__________________________________________________________


Alex Dixon, Ph.D. (He/Him)
Lab Manager
Nanofabrication and Thin Film Deposition
Shared Instrument Facility
Colorado School of Mines

________________________________
From: labnetwork <labnetwork-bounces at mtl.mit.edu> on behalf of Greg Allion <grallion at ncsu.edu>
Sent: Tuesday, March 4, 2025 3:37 PM
To: JAYER A FERNANDES <jfernandes at wisc.edu>
Cc: labnetwork at mtl.mit.edu <labnetwork at mtl.mit.edu>
Subject: [EXTERNAL] Re: [labnetwork] Photomask Manufacturing Companies

CAUTION: This email originated from outside of the Colorado School of Mines organization. Do not click on links or open attachments unless you recognize the sender and know the content is safe.

Hi Jayer,
If there's a reason we can't make them in house,  HTAphotomasks in Vegas is a good option.  https://www.htaphotomask.com/  Fast turn around, good prices.
We found them when photosciences was having some issues with response time.  https://photosciences.com/  No complaints with them prior to those issues.
There's a DWL 66 at the nanofab in Madison.  A good place for mask blanks is nanofilm.  https://www.nanofilm.com/
Contact me if you would like any more details.
Thanks,
Greg

On Tue, Mar 4, 2025 at 4:17 PM JAYER A FERNANDES <jfernandes at wisc.edu<mailto:jfernandes at wisc.edu>> wrote:
Hi,

I'm curious to know what service/company folks are using to make standard photomasks?

Regards



Jayer Fernandes

Micro/Nano Sensors and Actuators Laboratory (MNSA)
Department of Electrical and Computer Engineering
University of Wisconsin - Madison
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork


--
Greg Allion
NC State University Nanofabrication Facility (NNF)
Process Integration Engineering Manager

Monteith Research Center
2410 Campus Shore Drive rm.243F
Raleigh, NC 27606
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20250306/5e029753/attachment.html>


More information about the labnetwork mailing list