[labnetwork] Etching WO3
beaudoin
beaudoin at phas.ubc.ca
Mon Mar 17 16:47:39 EDT 2025
Thanks Darick,
And thanks to all fellow labnetworkers who responded.
Mario
On 2025-03-17 12:33, Darick Baker wrote:
> [CAUTION: Non-UBC Email]
>
> Hello Mario,
>
> Do you know how the WO3 is attached to the copper? You might be able
> to melt the solder or dissolve the epoxy that is holding the pieces
> together. That may be more pleasant than trying to etch the WO3.
> Good luck.
>
> On Fri, Mar 14, 2025 at 4:39 PM Beaudoin, Mario
> <beaudoin at physics.ubc.ca> wrote:
>
>> Dear Network,
>>
>> I have a big copper sputter target holder on which a WO3 (tungsten
>> tri-oxide) target on it. I'd like to etch away the WO3 and keep the
>> copper. Anyone can recommend some appropriate wet chemistry?
>>
>> Best
>>
>> Mario
>> --
>> _______________________________________________
>> labnetwork mailing list
>> labnetwork at mtl.mit.edu
>>
> https://urldefense.com/v3/__https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork__;!!K-Hz7m0Vt54!k9XMjkBayg2ou95ei1GayFpWTd64q2_R0KheTfu1ct5vp5WvO5TfgjOlFyDgGo30WD8Nhd0D-5wl7YZB0TTZbQ$
>
> --
>
> Darick Baker, PhD
> Manager, Engineering and Business Development
> Washington Nanofabrication Facility (WNF)
> University of Washington
> Fluke Hall 115, Box 352143
> Desk: 206.221.8265 Cell: 206.395.4049 (text preferred)
> https://www.wnf.washington.edu/
>
> Pronouns: he/him
--
Mario Beaudoin
More information about the labnetwork
mailing list