[labnetwork] Etching WO3

Darick Baker darick at uw.edu
Mon Mar 17 15:33:26 EDT 2025


Hello Mario,

Do you know how the WO3 is attached to the copper? You might be able to
melt the solder or dissolve the epoxy that is holding the pieces together.
That may be more pleasant than trying to etch the WO3.
Good luck.

On Fri, Mar 14, 2025 at 4:39 PM Beaudoin, Mario <beaudoin at physics.ubc.ca>
wrote:

> Dear Network,
>
> I have a big copper sputter target holder on which a WO3 (tungsten
> tri-oxide) target on it.  I'd like to etch away the WO3 and keep the
> copper.  Anyone can recommend some appropriate wet chemistry?
>
> Best
>
> Mario
> --
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
>
> https://urldefense.com/v3/__https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork__;!!K-Hz7m0Vt54!k9XMjkBayg2ou95ei1GayFpWTd64q2_R0KheTfu1ct5vp5WvO5TfgjOlFyDgGo30WD8Nhd0D-5wl7YZB0TTZbQ$
>


-- 
Darick Baker, PhD
Manager, Engineering and Business Development
Washington Nanofabrication Facility (WNF)
University of Washington
Fluke Hall 115, Box 352143
Desk: 206.221.8265 Cell: 206.395.4049 (text preferred)
https://www.wnf.washington.edu/
Pronouns: he/him
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20250317/0bcec7a0/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: Mario Beaudoin SBQMI sig 3.jpg
Type: image/jpeg
Size: 22413 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20250317/0bcec7a0/attachment.jpg>


More information about the labnetwork mailing list