We have a Raith EBPG 5150+ that was installed February 2024 that has had reoccurring holder movement issues since shortly after install that we can't seem to solve. I wanted to check in with other Raith 5150 owners to see if they have similar issues and have found any solutions. Raith has been out to service the holders and stage many times, and just spent three weeks doing the yearly PM and addressing this issue only to have it return two days after they left. Any other EBPG owners seeing similar issues? It manifests itself in "move marker: marker is not present in the search area" errors when loading the holders, or in abnormally large stitching errors if the holder is moving after the write has started.
Thanks for any insight anyone can share.
Dan
Daniel Woodie
Director, Micro/Nanofabrication Center, Princeton Materials Institute
Princeton University
155 Andlinger Center
86 Olden St
Princeton, NJ 08540
(609)258-5922 (office)
(607)227-2993 (cell)
daniel.woodie at princeton.edu<mailto:daniel.woodie at princeton.edu>
mnfc.princeton.edu<https://mnfc.princeton.edu/>
www.linkedin.com/in/danielpwoodie<http://www.linkedin.com/in/danielpwoodie/>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20250526/f66a467a/attachment.html>
More information about the labnetwork
mailing list