[labnetwork] Experience with Angstrom E-Beam Evaporators?

Srinivasan Raghavan sraghavan at iisc.ac.in
Wed Oct 22 22:23:41 EDT 2025


Hi Gabriel,


  *   In an academic setting the pump down time is important to increase throughput. We found that the Ferrotec tool, that has a large gate valve which isolates most of the volume while loading new samples, is very helpful in this regard. We had ebeam tools from other manufacturers and then got this Ferrotec tool which turned out be quite a blessing.
  *   Also, we found that it helps to get the ebeam tool from a vendor who also has control over the gun and its power supply. There are very few, Ferrotec being one. All the others get their guns and supplies and integrate them with a vacuum chamber.
  *   Having said that I have found Angstrom to be a fantastic company to work with. We have two of their sputtering units.
  *   We also have one from AJA which I have not heard any negative remarks about.
  *   Another point to keep in mind in cross contamination between pockets. Ferrotec has a pop up mechanism, whose details I had looked into when we procured the tool, and it made sense, compared to what the other supplies had.
  *   Lastly, one advantage of working with someone like Ferrotec is that they clam to have a good hold over the vapor phase flux distribution for most elements as they have been working with ebeams for a while. If you are going to be doing multiple wafers in a single run, helps with precious metal deposition, this becomes relevant to get uniformity across multiple wafers.
  *   A few things  I could think of.

Regards,
Srinivasan Raghavan (Vasu)
sraghavan at iisc.ac.in<mailto:sraghavan at iisc.ac.in>
Professor
Centre for Nano Science and Engineering (CeNSE)
IISc, Bengaluru, 560012, India

From: labnetwork <labnetwork-bounces at mtl.mit.edu> On Behalf Of Youry Borisenkov
Sent: 23 October 2025 05:47
To: Gabriel Catalano <gcatalano at stanford.edu>
Cc: labnetwork at mtl.mit.edu
Subject: Re: [labnetwork] Experience with Angstrom E-Beam Evaporators?

External Email

Hi Gabriel,
I double the previous referral.
We have two Angstrom ebeam tools (one older and one newer system) and they are great. Great tools and great service.
I never worked with Kj Lesker tools and we do have two AJAs sputtering systems. So I can’t comment on the e-beam performance. The sputtering tools are pretty sturdy and robust. The service tends to be a bit on the slow side, I think they might be bigger company (not sure about that) so it takes time to get the answers.
Hope this helps.
Youry


On Wed, Oct 22, 2025 at 8:05 PM Trieu Nguyen <trieu.nguyen at mail.wvu.edu<mailto:trieu.nguyen at mail.wvu.edu>> wrote:
Hi Gabe, Angstrom is a very good choice for PVD. They have provided very good service and have been highly responsive, replying to emails promptly and even offering free retraining when needed. Best regards, Trieu Nguyen, PhD Cleanroom(s) manager
ZjQcmQRYFpfptBannerStart
This Message Is From an External Sender
This message came from outside your organization.

ZjQcmQRYFpfptBannerEnd
Hi Gabe,

Angstrom is a very good choice for PVD. They have provided very good service and have been highly responsive, replying to emails promptly and even offering free retraining when needed.

Best regards,

Trieu Nguyen, PhD
Cleanroom(s) manager
Shared Research Facilities
West Virginia University
Office: WH 405 | ESB G60
Email: trieu.nguyen at mail.wvu.edu<mailto:trieu.nguyen at mail.wvu.edu>
Google Scholar: https://scholar.google.com/citations?user=SuHeFCAAAAAJ&hl=en<https://urldefense.com/v3/__https:/scholar.google.com/citations?user=SuHeFCAAAAAJ&hl=en__;!!BDUfV1Et5lrpZQ!UP_tn9x3KYyg5itoeWiYYePgZm5c53OmiGFVCCCQj_NTPOXNfiSZ8F-XaS6CGxjP1N_GuOM0KanGWYEA39JRkRGMaTDsAq7FRg$>
C: 916 532 4710
O: 304 293 5847

From: labnetwork <labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu>> On Behalf Of Peter Lomax
Sent: Wednesday, October 22, 2025 8:20 AM
To: Nathan Fitzpatrick <nnelsonfitzpatrick at uwaterloo.ca<mailto:nnelsonfitzpatrick at uwaterloo.ca>>; Gabriel Catalano <gcatalano at stanford.edu<mailto:gcatalano at stanford.edu>>; labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
Subject: Re: [labnetwork] Experience with Angstrom E-Beam Evaporators?

Hi Gabe,

We have both a sputter and e-beam evaporator.  We’ve been really impressed with both the equipment and the service – despite us being in Scotland.

The equipment is very easy to use with similar software.

Best

Peter

From: labnetwork <labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu>> On Behalf Of Nathan Fitzpatrick
Sent: 21 October 2025 22:28
To: Gabriel Catalano <gcatalano at stanford.edu<mailto:gcatalano at stanford.edu>>; labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
Subject: Re: [labnetwork] Experience with Angstrom E-Beam Evaporators?

You don't often get email from nnelsonfitzpatrick at uwaterloo.ca<mailto:nnelsonfitzpatrick at uwaterloo.ca>. Learn why this is important<https://urldefense.com/v3/__https:/aka.ms/LearnAboutSenderIdentification__;!!BDUfV1Et5lrpZQ!UP_tn9x3KYyg5itoeWiYYePgZm5c53OmiGFVCCCQj_NTPOXNfiSZ8F-XaS6CGxjP1N_GuOM0KanGWYEA39JRkRGMaTAB9uXNBQ$>
Hi Gabe,

Angstrom is a very good choice for PVD hardware.  Our lab has 4 Angstrom systems (1 E-beam, 2 Thermal, 1 LPCVD) and we are quite happy with our purchases.  They have been a very good partner for our lab.  We also benefit greatly by having local support since Angstrom is 30 minutes away from my office.

Nothing in the equipment world is perfect, but I would be happy to talk openly (offline) about Angstrom’s strengths and weaknesses.  I’m somewhat to very familiar with the offerings from the other vendors on your list as well.  I think everyone you are looking at is good.

Best,
  -Nathan


--

Nathan Fitzpatrick  PhD, PEng   (He/Him)

Director, Quantum-Nano Fabrication and Characterization Facility (QNFCF)

Office of Research

University of Waterloo

200 University Avenue West,<https://www.google.com/maps/search/200+University+Avenue+West,+Waterloo,+ON++N2L+3G1?entry=gmail&source=g> Waterloo, ON <https://www.google.com/maps/search/200+University+Avenue+West,+Waterloo,+ON++N2L+3G1?entry=gmail&source=g>  N2L 3G1<https://www.google.com/maps/search/200+University+Avenue+West,+Waterloo,+ON++N2L+3G1?entry=gmail&source=g>

P: 519-888-4567 ext. 31796

C: 226-218-3206

https://uwaterloo.ca/qnfcf/<https://urldefense.com/v3/__https:/uwaterloo.ca/quantum-nano-fabrication-and-characterization-facility/__;!!BDUfV1Et5lrpZQ!UP_tn9x3KYyg5itoeWiYYePgZm5c53OmiGFVCCCQj_NTPOXNfiSZ8F-XaS6CGxjP1N_GuOM0KanGWYEA39JRkRGMaTBljFbUDw$>



[cid:image001.png at 01DC43F2.23E6FF00]
From: labnetwork <labnetwork-bounces at mtl.mit.edu<mailto:labnetwork-bounces at mtl.mit.edu>> on behalf of Gabriel Catalano <gcatalano at stanford.edu<mailto:gcatalano at stanford.edu>>
Date: Monday, October 20, 2025 at 9:31 PM
To: labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu> <labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>>
Subject: [labnetwork] Experience with Angstrom E-Beam Evaporators?
Hello All,

We are in the process of procuring a new E-Beam evaporator and considering options from Kurt J. Lesker, AJA Internation, and Angstrom Engineering; the pricing between all three vendors is comparable. We have lots experience using and maintaining KJL and AJA systems, but do not have much exposure to Angstrom Engineering's systems. We are curious for other nanolabs experience with these tools, particularly from a maintenance prospective. We plan to use this tool for both metal and oxide depositions. Any feedback or thoughts on Angstrom's E-beam systems is very much appreciated!

Kind Regards,
------------------------
Gabe Catalano
Lab Operations
Stanford Nanofabrication Facility (SNF)
(650) 498-4014
https://snf.stanford.edu/<https://urldefense.com/v3/__https:/snf.stanford.edu/__;!!BDUfV1Et5lrpZQ!UP_tn9x3KYyg5itoeWiYYePgZm5c53OmiGFVCCCQj_NTPOXNfiSZ8F-XaS6CGxjP1N_GuOM0KanGWYEA39JRkRGMaTBeG8Sh3Q$>

The University of Edinburgh is a charitable body, registered in Scotland, with registration number SC005336. Is e buidheann carthannais a th’ ann an Oilthigh Dhùn Èideann, clàraichte an Alba, àireamh clàraidh SC005336.
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://urldefense.com/v3/__https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork__;!!BDUfV1Et5lrpZQ!UP_tn9x3KYyg5itoeWiYYePgZm5c53OmiGFVCCCQj_NTPOXNfiSZ8F-XaS6CGxjP1N_GuOM0KanGWYEA39JRkRGMaTBN8h8Xrw$<https://urldefense.com/v3/__https:/mtl.mit.edu/mailman/listinfo.cgi/labnetwork__;!!BDUfV1Et5lrpZQ!UP_tn9x3KYyg5itoeWiYYePgZm5c53OmiGFVCCCQj_NTPOXNfiSZ8F-XaS6CGxjP1N_GuOM0KanGWYEA39JRkRGMaTBN8h8Xrw$>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20251023/217aa154/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 16335 bytes
Desc: image001.png
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20251023/217aa154/attachment.png>


More information about the labnetwork mailing list