[labnetwork] Dicing Diamond?

Demis D. John demis at ucsb.edu
Wed Aug 12 14:59:52 EDT 2026


Thanks for the responses everyone - I'll let you know what our lab user
figures out for this.

-- Demis (contact info <https://wiki.nanotech.ucsb.edu/wiki/Demis_D._John>)
*Reminder*: The NanoFab has a publications policy
<https://wiki.nanotech.ucsb.edu/wiki/Frequently_Asked_Questions#Publications_acknowledging_the_Nanofab>


On Wed, Aug 12, 2026 at 10:40 AM Martin, Michael <
michael.martin at louisville.edu> wrote:

> Hi Demis,
>     We had a synthetic diamond company adjacent to our campus that made
> thick crystals. I believe they just used a solid-state laser to cut them
> up.  I don't think it was anything exotic in terms of wavelength.
> Somewhere in the IR, I think.
>
> -Michael
> ------------------------------
> *From:* labnetwork <labnetwork-bounces at mtl.mit.edu> on behalf of Demis D.
> John <demis at ucsb.edu>
> *Sent:* Monday, August 10, 2026 10:53 PM
> *To:* labnetwork <labnetwork at mtl.mit.edu>
> *Subject:* [labnetwork] Dicing Diamond?
>
>
> *CAUTION:* This email originated from outside of our organization. Do not
> click links, open attachments, or respond unless you recognize the sender's
> email address and know the contents are safe.
> Does anyone have a recipe for dicing 500μm thick Diamond substrates?
> Is such a thing even possible (I assume Diamond Grit vs. Diamond Substrate
> is a losing proposition?)
>
> Let me know how you've handled this situation if it's come up - eg. Laser
> dicing (stealth/cutting) @ Disco service perhaps?
>
> Thanks!
> -- Demis
>
> ----------------------------------------
> *     Process Group Manager*
>  *UCSB Nanofabrication Facility* <https://www.nanotech.ucsb.edu/>
>          Demis' Contact Info
> <https://wiki.nanotech.ucsb.edu/wiki/Demis_D._John>
> ----------------------------------------
> *Reminder*: The NanoFab has a publications policy
> <https://wiki.nanotech.ucsb.edu/wiki/Frequently_Asked_Questions#Publications_acknowledging_the_Nanofab>
>
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20260812/609037bf/attachment.html>


More information about the labnetwork mailing list