Hi Alex,
Another option:
https://www.golighthouse.com/en/airborne-particle-counters/
iulian Codreanu, Ph.D.
Director, Nanofabrication Facility
University of Delaware
Harker ISE Lab, Room 163
221 Academy Street
Newark, DE 19716
302-831-2784
https://udnf.udel.edu
On 3/23/2026 4:21 PM, Alex Dixon wrote:
> Hi Everyone, I was wondering what people use for particle measurement
> systems in their cleanrooms? We are trying to add active particle
> monitoring to our cleanroom facilities. I was looking at the lasair
> pro from "Particle Measuring Systems" https://www.pmeasuring.com/ but
> university procurement is asking me to put together some other options.
>
> -Alex
>
> __________________________________________________________
>
>
> Alex Dixon, Ph.D. (He/Him)
> Lab Manager
> Nanofabrication and Thin Film Deposition
> Shared Instrument Facility
> Colorado School of Mines
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20260324/162d0a63/attachment.html>
More information about the labnetwork
mailing list