[labnetwork] 100% Silane Bottle Changing
Charles Ellis
elliscd at auburn.edu
Mon Jun 10 20:14:32 EDT 2013
We run 4% silane - takes a little longer, but the films look good and much less dangerous.
On Jun 10, 2013, at 6:53 PM, "Aebersold,Julia W." <julia.aebersold at louisville.edu<mailto:julia.aebersold at louisville.edu>> wrote:
We are hooking up a new polysilicon tube and are working with 100% Silane. I am seeking information on protocol and standard operating procedures (SOP’s) on how other groups and institutions perform this the process of changing their Silane bottle and leak checks. We have our gas cabinet information, but due to the dangerous nature of this gas more I would like to gather information from other folks that have worked with this gas extensively.
A written response to my e-mail is fine, but links to sites with official protocol and SOP’s would be preferred.
Cheers!
Julia Aebersold, Ph.D.
MNTC Cleanroom Manager
Shumaker Research Building, Room 233
2210 South Brook Street
University of Louisville
Louisville, KY 40292
502-852-1572
http://louisville.edu/micronano/
_______________________________________________
labnetwork mailing list
labnetwork at mtl.mit.edu<mailto:labnetwork at mtl.mit.edu>
https://www-mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20130611/71ee0e08/attachment.html>
More information about the labnetwork
mailing list