Hi Nava,
We recently got a vacuum muffle furnace from SH Scientific that meets all
of those requirements (not sure about the 20deg/min ramp rate).
We have only used it a handful of times, but we are pleased with its
performance so far.
My contact person there is JH Bang (jhbang at samheung21.c
<jhbang at samheung21.com>om).
Brian

--

______________
Brian Little, Ph.D.
Senior Research Scholar
Electrical and Computer Engineering Department
Campus Box 7911
2410 Campus Shore Drive, Room 322F
Monteith Engineering Research Center (MRC)
Raleigh, NC 27606
Email: bdlittl2 at ncsu.edu
Mobile: 919-272-4984

On Fri, Jun 7, 2024 at 5:20 PM Nava Ariel-Sternberg <na2661 at columbia.edu>
wrote:

> Dear wise Yodas of the cleanroom,
>
> We are looking for vendors that can sell us an anneal furnace for single
> or more 4” wafer processing (and pieces). The furnace needs to get to
> 1,200C with temperature ramp rate of 5-20 deg/min. It should have the
> options of rough vacuum and anneal atmospheres of Ar, N2, or O2.
>
> Thanks,
>
> Nava
>
> Dr. Nava Ariel-Sternberg
>
> Senior Director of CNI Labs
>
> Columbia University
>
> CEPSR/MC 8903
>
> 530 west 120th st. NY
>
> NY 10027
>
> Office: 212-8549927
>
> Cell: 201-5627600
>
> [image:
> https://sustainable.columbia.edu/sites/default/files/content/crown%20commuter%20badge_1.png]
>
>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20240607/71434665/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 9094 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20240607/71434665/attachment.png>


More information about the labnetwork mailing list