[labnetwork] SU-8 distributors (Kayaku ending SU-8 2000 series early 2025)

Eric Johnston ericdj at seas.upenn.edu
Wed Oct 30 10:21:48 EDT 2024


Hi Ben

We have been working with Kem Lab recently. They offer their version of SU8
and Jeremy Golden has been very helpful.

My understanding is that the surfactants that have been used in these types
of resist are on the verge of being banned, as they are the same or similar
to PFAS. Please, anyone feel free to correct me on this!

Regarding your specific question, we have experience with SU8 3000, which
offers better adhesion at the cost of slightly poorer resolution.

Best

Eric

Eric Johnston
Director, Quattrone Nanofabrication Facility
Singh Center for Nanotechnology
University of Pennsylvania
3205 Walnut Street, #109A
ericdj at seas.upenn.edu
T. 215.573.6695
Questions? Start here
<https://wiki.nano.upenn.edu/wiki/index.php?title=Frequently_Asked_Questions#How_do_I_get_started.3F>
.

On Wed, Oct 23, 2024 at 9:27 PM Schmidt, Benjamin Willis <
ben.w.schmidt at vanderbilt.edu> wrote:

> Hello labnetwork,
>
>
>
> I have two questions:
>
>
>
>    1. We recently received notice from Kayaku Advanced Materials they
>    would stop distribution of SU-8 2000 series resists in early 2025.  Is
>    anyone aware of alternate suppliers?
>    2. They have recommended new options based on desired thickness: <10
>    um (SU-8 3000, SU-8 TF 6000 series), 10 – 50 um (SU-8 3000 series), >50 um
>    (SU-8 XFT75, SU-8 XFT100). Does anyone have experience with these in
>    comparison to the 2000 series?  We assume we would need to redo our recipes
>    but hoped to get some general insight from others.
>
>
>
> Lastly, I used nanobot.chat to find a previous thread in the labnetwork
> archives from 2021.  Is there a way to reply directly to that thread to
> keep the conversation together?  I couldn’t find anything so that’s why I’m
> starting a fresh one now.
>
> https://mtl.mit.edu/pipermail/labnetwork/2021-January/004537.html
> <https://urldefense.com/v3/__https://mtl.mit.edu/pipermail/labnetwork/2021-January/004537.html__;!!IBzWLUs!UZHyeAIw2_pekj2hXTqmxyP2sM302kYFrNLwBz8kSSoJBYLz8ZVl5L4TEjby0_L-f_9LrT7qBxFpaDQ9O_euQ7RGxCWnqR70Dw$>
>
>
>
> Thanks for your help,
>
> Ben
>
>
>
>
>
>
>
> [image: Vanderbilt]
>
>
>
> Ben W. Schmidt, Ph.D.
>
> Cleanroom Manager
> Vanderbilt Institute of Nanoscale Science and Engineering
>
> Vanderbilt University, Nashville, TN
> 615.875.9294 | ben.schmidt at vanderbilt.edu | vu.edu/vinse
> <https://urldefense.com/v3/__https://www.vanderbilt.edu/vinse/__;!!IBzWLUs!UZHyeAIw2_pekj2hXTqmxyP2sM302kYFrNLwBz8kSSoJBYLz8ZVl5L4TEjby0_L-f_9LrT7qBxFpaDQ9O_euQ7RGxCUfl7iKVQ$>
>
> Book time with Schmidt, Benjamin Willis
> <https://urldefense.com/v3/__https://outlook.office.com/bookwithme/user/4be23d791b054cfab7650ff91ba047e2@Vanderbilt.Edu?anonymous&ep=pcard__;!!IBzWLUs!UZHyeAIw2_pekj2hXTqmxyP2sM302kYFrNLwBz8kSSoJBYLz8ZVl5L4TEjby0_L-f_9LrT7qBxFpaDQ9O_euQ7RGxCW7GPngdg$>
>
>
>  [image: Twitter]
> <https://urldefense.com/v3/__https://twitter.com/VanderbiltVinse__;!!IBzWLUs!UZHyeAIw2_pekj2hXTqmxyP2sM302kYFrNLwBz8kSSoJBYLz8ZVl5L4TEjby0_L-f_9LrT7qBxFpaDQ9O_euQ7RGxCU_doxieQ$>
>  [image: Facebook]
> <https://urldefense.com/v3/__https://www.facebook.com/VINSE.Vanderbilt__;!!IBzWLUs!UZHyeAIw2_pekj2hXTqmxyP2sM302kYFrNLwBz8kSSoJBYLz8ZVl5L4TEjby0_L-f_9LrT7qBxFpaDQ9O_euQ7RGxCWDp59suQ$>
>  [image: Instagram]
> <https://urldefense.com/v3/__https://www.instagram.com/vinsetagram/__;!!IBzWLUs!UZHyeAIw2_pekj2hXTqmxyP2sM302kYFrNLwBz8kSSoJBYLz8ZVl5L4TEjby0_L-f_9LrT7qBxFpaDQ9O_euQ7RGxCUKbu7ftQ$>
>  [image: LinkedIn]
> <https://urldefense.com/v3/__https://www.linkedin.com/company/vinse/__;!!IBzWLUs!UZHyeAIw2_pekj2hXTqmxyP2sM302kYFrNLwBz8kSSoJBYLz8ZVl5L4TEjby0_L-f_9LrT7qBxFpaDQ9O_euQ7RGxCXVlw5f4A$>
>  [image: YouTube]
> <https://urldefense.com/v3/__https://www.youtube.com/playlist?list=PLB1EPeYUwa4mwVbt2dweqUzD8Xy2ZWgeT__;!!IBzWLUs!UZHyeAIw2_pekj2hXTqmxyP2sM302kYFrNLwBz8kSSoJBYLz8ZVl5L4TEjby0_L-f_9LrT7qBxFpaDQ9O_euQ7RGxCWiWQNWGQ$>
>
>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
>
> https://urldefense.com/v3/__https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork__;!!IBzWLUs!UZHyeAIw2_pekj2hXTqmxyP2sM302kYFrNLwBz8kSSoJBYLz8ZVl5L4TEjby0_L-f_9LrT7qBxFpaDQ9O_euQ7RGxCVnwyOgzg$
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20241030/4a874dc1/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 10049 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20241030/4a874dc1/attachment.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image002.png
Type: image/png
Size: 1359 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20241030/4a874dc1/attachment-0001.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image003.png
Type: image/png
Size: 951 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20241030/4a874dc1/attachment-0002.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image004.png
Type: image/png
Size: 1387 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20241030/4a874dc1/attachment-0003.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image005.png
Type: image/png
Size: 1109 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20241030/4a874dc1/attachment-0004.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image006.png
Type: image/png
Size: 752 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20241030/4a874dc1/attachment-0005.png>


More information about the labnetwork mailing list