[labnetwork] Experience with Angstrom E-Beam Evaporators?

Soltanian s.soltanian at gmail.com
Tue Oct 21 11:33:47 EDT 2025


Hello Gabel,
In our lab at CFET, we have two Angstrom Engineering systems (one is
sputtering, and the other is an Ebeam and resistive evaporator). We are
very happy with them. Their after-sales support and maintenance are
excellent. They were very accommodating with customizing the system based
on our needs. Happy to have a chat with you and/or provide more information
if needed.
Best,
Saeid

-- Saeid Soltanian, PhD Research Associate, Manager Centre for Flexible
Electronics and Textiles (CFET) University of British Columbia 117-2355
East Mall, Vancouver, BC V6T 1Z4 Tel: +1-604-827-1573 Email:
saeid.soltanian at ubc.ca http://cfet.ubc.ca/

On Mon, Oct 20, 2025 at 6:32 PM Gabriel Catalano <gcatalano at stanford.edu>
wrote:

> Hello All,
>
> We are in the process of procuring a new E-Beam evaporator and considering
> options from Kurt J. Lesker, AJA Internation, and Angstrom Engineering; the
> pricing between all three vendors is comparable. We have lots experience
> using and maintaining KJL and AJA systems, but do not have much exposure to
> Angstrom Engineering's systems. We are curious for other nanolabs
> experience with these tools, particularly from a maintenance prospective.
> We plan to use this tool for both metal and oxide depositions. Any feedback
> or thoughts on Angstrom's E-beam systems is very much appreciated!
>
> Kind Regards,
> ------------------------
> *Gabe Catalano*
> Lab Operations
> Stanford Nanofabrication Facility (SNF)
> (650) 498-4014
> https://snf.stanford.edu/
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20251021/68478871/attachment.html>


More information about the labnetwork mailing list