Good afternoon,
Here at the University of New Mexico we have 2 Osiris table top HMDS ovens.
They have both failed for different reasons. My attempts to gather information from the manufacturer has been met with little information and
then no replies at all. I have schematics, which help. Does anyone else use these ovens? Have you had issues with them?
While I am trying to fix the problems with these, my director would like information on other table top units.
I look forward to responses.

Best regards,

Mark Hofheins



mhofheins at unm.edu<mailto:mhofheins at unm.edu>

Cell  505-259-9278

Office 505-272-7506



Micro Electronics Technician &

 Safety Coordinator MTTC

Manufacturing Engineering/

School of Engineering

Science and Technology park

University of New Mexico

800 Bradbury S.E.  Suit 169

Albuquerque, New Mexico

87106-4346

-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20260403/3b499ff6/attachment.html>


More information about the labnetwork mailing list