[labnetwork] Evaporating Iridium
Gila,Brent P
bgila at ufl.edu
Tue Aug 4 17:27:01 EDT 2026
Hello Jason,
Due to its really high temperature to evaporate and slow deposition
rate, we purchased a sputter target. Works great!
You just have to take out a loan to afford the target.
Best Regards,
Brent
On 8/4/2026 1:18 PM, Oncel, Nuri wrote:
> *[External Email]*
>
> Hi Jason,
> I have deposited Ir on a variety of surfaces, and the process is
> actually quite straightforward. I simply connected an Ir wire to a
> high current feedthrough (connected to a UHV STM chamber) and passed
> the current through it to evaporate the metal. I calibrated the
> deposition rate using Auger.
> A common approach is to use a W wire and wrap the source material
> around it. However, that method can also result in some W being
> co-deposited along with Iridium.
> For your reference, I've attached three of my papers that mention Ir
> deposition.
> Please feel free to reach out if you have any questions or if there's
> anything else I can help with.
> Best,
> Nuri
>
>
> Professor Nuri Oncel, Ph.D.
>
> _Director of UND-NanoFoundry_
> <https://www.und.edu/Nanofoundry>
>
> Department of Physics and Astrophysics
>
> University of North Dakota
>
> _https://sites.google.com/view/oncel-research-group/group_
> <https://sites.google.com/view/oncel-research-group/group>
>
> ------------------------------------------------------------------------
> *From:* labnetwork <labnetwork-bounces at mtl.mit.edu> on behalf of
> EDWARDS, JASON R CTR USAF AFMC AFRL/RYDD <jason.edwards.30.ctr at us.af.mil>
> *Sent:* Tuesday, August 4, 2026 8:09 AM
> *To:* labnetwork at mtl.mit.edu <labnetwork at mtl.mit.edu>
> *Subject:* [labnetwork] Evaporating Iridium
>
> Good morning network,
>
> I am interested to see if any of you have experience using Iridium in
> your evaporation systems. We are getting conflicting information from
> various manufacturers on how we should go about melting our Iridium.
> Our OEM recommends melting straight in the pocket while Lesker
> recommends using their Fabmate crucible liner. If you evaporate
> Iridium, do you use a liner in your system? In what form do you
> receive your Iridium? Pellets, shot, rods? For what it is worth the
> Iridium that was purchased for us is flat fractured pieces ranging in
> size from dust to 8mm, which seems less than ideal.
>
> Thanks,
>
>
>
> *Jason Edwards*
>
> Clean Room Facilities Manager | National Security Solutions
>
> KBR | Mission Technology Solutions
>
> 2241 Avionics Circle, Area B, Bldg.600|WPAFB, OH, 45433 | USA
>
> Office: +1 937.713.8741 | Mobile: +1 937.524.7701
>
> Jason.edwards.30.ctr at us.af.mil
> <http://Jason.edwards.30.ctr@us.af.mil/>
>
> <https://www.facebook.com/pages/KBR-Inc/153705171306696><https://twitter.com/KBRincorporated><https://www.linkedin.com/company/kbr-inc><https://instagram.com/kbr.inc>
>
>
> _______________________________________________
> labnetwork mailing list
> labnetwork at mtl.mit.edu
> https://mtl.mit.edu/mailman/listinfo.cgi/labnetwork
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20260804/45e44cb0/attachment.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: UF email signature 2026.png
Type: image/png
Size: 11618 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20260804/45e44cb0/attachment.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image001.png
Type: image/png
Size: 5577 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20260804/45e44cb0/attachment-0001.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image002.png
Type: image/png
Size: 584 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20260804/45e44cb0/attachment-0002.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image003.png
Type: image/png
Size: 660 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20260804/45e44cb0/attachment-0003.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image004.png
Type: image/png
Size: 715 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20260804/45e44cb0/attachment-0004.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: image005.png
Type: image/png
Size: 901 bytes
Desc: not available
URL: <https://mtl.mit.edu/pipermail/labnetwork/attachments/20260804/45e44cb0/attachment-0005.png>
More information about the labnetwork
mailing list